Steel A48 Class 20-ANN vs A48 Class 20-FH

Steel · A48 Class 20 temper comparison

A48 Class 20-ANN and A48 Class 20-FH are two conditions of the same steel grade, A48 Class 20: ANN (annealed) versus FH (full hard). The chemistry is identical, so every difference below comes from the condition. A48 Class 20-FH is the stronger of the two: tensile strength 152 MPa (22 ksi) against 135 MPa (19.6 ksi) for A48 Class 20-ANN, about 13% more. In exchange, A48 Class 20-ANN is the more ductile: elongation 0.8% versus 0.3% for A48 Class 20-FH, and A48 Class 20-FH is harder (156 HB vs 125 HB). A48 Class 20-ANN runs hotter in service (350°C vs 250°C continuous). On the shop floor, A48 Class 20-ANN machines more easily (excellent vs poor) and A48 Class 20-ANN welds better (fair vs not recommended).

A48 Class 20-ANNChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

A48 Class 20-FHChoose it when strength drives the design.

A48 Class 20-ANN vs A48 Class 20-FH: properties

A48 Class 20-ANNA48 Class 20-FH

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

78 GPa11.3 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

135 MPa19.6 ksi
152 MPa22 ksi

Elongation at Break

0.8%
0.3%

Compressive Strength

520 MPa75.4 ksi
600 MPa87 ksi

Shear Strength

160 MPa23.2 ksi
185 MPa26.8 ksi

Fatigue Strength (Endurance Limit)

62 MPa9 ksi
95 MPa13.8 ksi

Fracture Toughness (K_IC)

13 MPa·√m11.8 ksi·√in
11 MPa·√m10 ksi·√in

Hardness, Brinell

125 HB
156 HB

Hardness, Rockwell B

70 HRB
82 HRB

Hardness, Vickers

130 HV
450 HV

Same in both: Shear Modulus 32 GPa4.6 Msi · Bulk Modulus 56 GPa8.1 Msi · Poisson's Ratio 0.26

Physical

Density and transition temperatures.

Same in both: Density 7.1 g/cm³0.26 lb/in³ · Melting Point (Solidus) 1,150°C2,102 °F · Liquidus Temperature 1,175°C2,147 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

55 W/m·K31.8 BTU/hr·ft·°F
52 W/m·K30 BTU/hr·ft·°F

Max Service Temperature (continuous)

350°C662 °F
250°C482 °F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.4 µm/m·K6.3 µin/in·°F · Latent Heat of Fusion 220 J/g94.6 BTU/lb · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.3 % IACS
2.2 % IACS

Electrical Resistivity

7.7×10⁻⁷ Ω·m30.3 µΩ·in
8.2×10⁻⁷ Ω·m32.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

18 / 100
20 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

95 / 100
25 / 100

Machinability Rating (AISI 1212 = 100 %)

140%
20%

Weldability

35 / 100
10 / 100

Formability (cold)

4 / 100
1 / 100

Same in both: Castability 96 / 100 · Brazeability / Solderability 50 / 100 · Polishability 30 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 17 MJ/kg7,309 BTU/lb · Embodied Carbon (primary production) 1.6 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale

A48 Class 20-ANN vs A48 Class 20-FH — frequently asked

Is A48 Class 20-FH stronger than A48 Class 20-ANN?

Yes. A48 Class 20-FH has a typical tensile strength of 152 MPa (22 ksi) against 135 MPa (19.6 ksi) for A48 Class 20-ANN — about 13% more.

Which condition does FabDigit quote by default, ANN or FH?

F is the default A48 Class 20 condition in the FabDigit quote flow (neither ANN nor FH). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, A48 Class 20-ANN or A48 Class 20-FH?

A48 Class 20-ANN. Its machinability rates excellent (95/100) against poor (25/100) for A48 Class 20-FH; for welding the order is A48 Class 20-ANN first (fair, 35/100) then A48 Class 20-FH (not recommended, 10/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in A48 Class 20-ANN and A48 Class 20-FH side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.