4817-A and 4817-HR are two conditions of the same steel grade, 4817: A (solution annealed) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. Both yield at about 450 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (solution annealed versus hot rolled). 4817-HR is harder — 207 HB against 195 HB for 4817-A — which matters for wear surfaces and threads.

4817-HRChoose it when surface hardness matters.

4817-A vs 4817-HR: properties

4817-A4817-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

690 MPa100 ksi
720 MPa104 ksi

Yield Strength (0.2% offset)

450 MPa65.3 ksi
440 MPa63.8 ksi

Elongation at Break

24%
22%

Reduction in Area

55%
50%

Shear Strength

450 MPa65.3 ksi
470 MPa68.2 ksi

Fatigue Strength (Endurance Limit)

330 MPa47.9 ksi
340 MPa49.3 ksi

Fracture Toughness (K_IC)

85 MPa·√m77.4 ksi·√in
80 MPa·√m72.8 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
75 J55.3 ft·lbf

Hardness, Brinell

195 HB
207 HB

Hardness, Rockwell B

92 HRB
94 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.83 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 33 W/m·K19.1 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 260 J/g112 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -70°C-94 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Resistivity 2.5×10⁻⁷ Ω·m9.84 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 13 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
50%

Formability (cold)

45 / 100
42 / 100

Same in both: Weldability 35 / 100 · Brazeability / Solderability 55 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 34 MJ/kg14,617 BTU/lb · Embodied Carbon (primary production) 2.5 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4817

4817-A vs 4817-HR — frequently asked

What is the difference between 4817-A and 4817-HR?

4817-A and 4817-HR are two conditions of the same steel grade, 4817: A (solution annealed) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. Both yield at about 450 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (solution annealed versus hot rolled).

Which condition does FabDigit quote by default, A or HR?

A is the default 4817 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 4817-A or 4817-HR?

4817-A, by a small margin. Both rate fair for machinability — 45/100 against 40/100 for 4817-HR.