FabDigitFabDigit

Steel 45#-CD vs 45# Normalized

Steel · 45# temper comparison

45#-CD and 45# Normalized are two conditions of the same steel grade, 45#: CD (cold drawn) versus Normalized. The chemistry is identical, so every difference below comes from the condition. 45#-CD is the stronger of the two: yield strength 530 MPa (76.9 ksi) against 375 MPa (54.4 ksi) for 45# Normalized, about 41% more. In exchange, 45# Normalized is the more ductile: elongation 18% versus 12% for 45#-CD.

45#-CDChoose it when strength drives the design.

45# NormalizedChoose it when the part is bent, formed or impact-loaded.

45#-CD vs 45# Normalized: properties

45#-CD45# Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

625 MPa90.6 ksi
630 MPa91.4 ksi

Yield Strength (0.2% offset)

530 MPa76.9 ksi
375 MPa54.4 ksi

Elongation at Break

12%
18%

Reduction in Area

35%
42%

Shear Strength

400 MPa58 ksi
410 MPa59.5 ksi

Fatigue Strength (Endurance Limit)

310 MPa45 ksi
290 MPa42.1 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in
62 MPa·√m56.4 ksi·√in

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
40 J29.5 ft·lbf

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Compressive Strength 540 MPa78.3 ksi · Hardness, Brinell 179 HB · Hardness, Rockwell B 89 HRB · Hardness, Vickers 188 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 49 W/m·K28.3 BTU/hr·ft·°F · Specific Heat Capacity 486 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 425°C797 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10.8 % IACS · Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Weldability

44 / 100
46 / 100

Formability (cold)

30 / 100
38 / 100

Same in both: Machinability 56 / 100 · Machinability Rating (AISI 1212 = 100 %) 57% · Brazeability / Solderability 60 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale45#

45#-CD vs 45# Normalized — frequently asked

Is 45#-CD stronger than 45# Normalized?

Yes. 45#-CD has a typical yield strength of 530 MPa (76.9 ksi) against 375 MPa (54.4 ksi) for 45# Normalized — about 41% more. Tensile strength is 625 MPa (90.6 ksi) vs 630 MPa (91.4 ksi).

Which condition does FabDigit quote by default, CD or Normalized?

CD is the default 45# condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose 45#-CD over 45# Normalized?

Pick 45#-CD when strength drives the design. Pick 45# Normalized when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 45#-CD and 45# Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.