45#-A and 45#-CD are two conditions of the same steel grade, 45#: A (solution annealed) versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. 45#-CD is the stronger of the two: yield strength 530 MPa (76.9 ksi) against 340 MPa (49.3 ksi) for 45#-A, about 56% more; tensile strength follows at 625 MPa (90.6 ksi) vs 570 MPa (82.7 ksi). In exchange, 45#-A is the more ductile: elongation 22% versus 12% for 45#-CD, and 45#-CD is harder (179 HB vs 163 HB).

45#-AChoose it when the part is bent, formed or impact-loaded.

45#-CDChoose it when strength drives the design.

45#-A vs 45#-CD: properties

45#-A45#-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

570 MPa82.7 ksi
625 MPa90.6 ksi

Yield Strength (0.2% offset)

340 MPa49.3 ksi
530 MPa76.9 ksi

Elongation at Break

22%
12%

Reduction in Area

50%
35%

Fatigue Strength (Endurance Limit)

260 MPa37.7 ksi
310 MPa45 ksi

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
20 J14.8 ft·lbf

Hardness, Brinell

163 HB
179 HB

Hardness, Rockwell B

84 HRB
89 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Compressive Strength 540 MPa78.3 ksi · Shear Strength 400 MPa58 ksi · Fracture Toughness (K_IC) 60 MPa·√m54.6 ksi·√in · Hardness, Vickers 188 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 49 W/m·K28.3 BTU/hr·ft·°F · Specific Heat Capacity 486 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 425°C797 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10.8 % IACS · Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
56 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
57%

Weldability

50 / 100
44 / 100

Formability (cold)

50 / 100
30 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale45#

45#-A vs 45#-CD — frequently asked

Is 45#-CD stronger than 45#-A?

Yes. 45#-CD has a typical yield strength of 530 MPa (76.9 ksi) against 340 MPa (49.3 ksi) for 45#-A — about 56% more. Tensile strength is 625 MPa (90.6 ksi) vs 570 MPa (82.7 ksi).

Which condition does FabDigit quote by default, A or CD?

CD is the default 45# condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 45#-A or 45#-CD?

45#-A. Its weldability rates fair (50/100) against fair (44/100) for 45#-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 45#-A and 45#-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.