S44800 Annealed and S44800 As Welded are two conditions of the same stainless steel grade, S44800: Annealed versus As Welded (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 480 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (Annealed versus as-welded deposit). S44800 Annealed is the more ductile: elongation 25% versus 15% for S44800 As Welded.
S44800 AnnealedChoose it when the part is bent, formed or impact-loaded.
S44800 Annealed vs S44800 As Welded: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all stainless steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all stainless steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
S44800 AnnealedS44800 As Welded
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Tensile Strength (Ultimate)
Yield Strength (0.2% offset)
Elongation at Break
Reduction in Area
Compressive Strength
Shear Strength
Fatigue Strength (Endurance Limit)
Charpy V-Notch Impact (RT)
Hardness, Brinell
Hardness, Rockwell B
Hardness, Vickers
Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29
Physical
Density and transition temperatures.
Same in both: Density 7.67 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,490°C2,714 °F
Thermal
How each material carries heat and how hot it can run.
Same in both: Thermal Conductivity 16 W/m·K9.2 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 10.4 µm/m·K5.8 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 300°C572 °F · Min Service Temperature -40°C-40 °F
Electrical
Conductivity and insulation.
Same in both: Electrical Conductivity 2.3 % IACS · Electrical Resistivity 7.6×10⁻⁷ Ω·m29.9 µΩ·in
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Corrosion Resistance
Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Machinability Rating (AISI 1212 = 100 %)
Weldability
Formability (cold)
Same in both: Brazeability / Solderability 55 / 100 · Polishability 70 / 100
Sustainability
Primary-production footprint per kilogram.
Same in both: Embodied Energy (primary production) 70 MJ/kg30,095 BTU/lb · Embodied Carbon (primary production) 5.2 kg CO₂/kg · Embodied Water 100 L/kg12 gal/lb · Typical Recycled Content 30%
Strength versus weight
Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
S44800 Annealed vs S44800 As Welded — frequently asked
What is the difference between S44800 Annealed and S44800 As Welded?
S44800 Annealed and S44800 As Welded are two conditions of the same stainless steel grade, S44800: Annealed versus As Welded (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 480 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (Annealed versus as-welded deposit).
Which condition does FabDigit quote by default, Annealed or As Welded?
Annealed is the default S44800 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.
Which welds better, S44800 Annealed or S44800 As Welded?
S44800 Annealed. Its weldability rates good (55/100) against fair (50/100) for S44800 As Welded.
Ready to make it?
Upload a CAD file and FabDigit prices the part in S44800 Annealed and S44800 As Welded side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.