S44625-ANN and S44625-AW are two conditions of the same stainless steel grade, S44625: ANN (annealed) versus AW (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 380 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (annealed versus as-welded deposit). S44625-ANN is the more ductile: elongation 28% versus 15% for S44625-AW, and S44625-AW is harder (185 HB vs 175 HB).

S44625-ANNChoose it when the part is bent, formed or impact-loaded.

S44625-ANN vs S44625-AW: properties

S44625-ANNS44625-AW

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

500 MPa72.5 ksi
490 MPa71.1 ksi

Yield Strength (0.2% offset)

380 MPa55.1 ksi
370 MPa53.7 ksi

Elongation at Break

28%
15%

Reduction in Area

60%
28%

Shear Strength

330 MPa47.9 ksi
320 MPa46.4 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
170 MPa24.7 ksi

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
7 J5.2 ft·lbf

Hardness, Brinell

175 HB
185 HB

Hardness, Rockwell B

88 HRB
90 HRB

Hardness, Vickers

185 HV
195 HV

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Compressive Strength 385 MPa55.8 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.67 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 20.5 W/m·K11.8 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 9.9 µm/m·K5.5 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 300°C572 °F · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 2.9 % IACS · Electrical Resistivity 6×10⁻⁷ Ω·m23.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

74 / 100
68 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

48 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
48%

Formability (cold)

60 / 100
25 / 100

Same in both: Weldability 55 / 100 · Brazeability / Solderability 65 / 100 · Polishability 62 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 90 L/kg10.8 gal/lb · Typical Recycled Content 45%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleS44625

S44625-ANN vs S44625-AW — frequently asked

What is the difference between S44625-ANN and S44625-AW?

S44625-ANN and S44625-AW are two conditions of the same stainless steel grade, S44625: ANN (annealed) versus AW (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 380 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (annealed versus as-welded deposit).

Which condition does FabDigit quote by default, ANN or AW?

ANN is the default S44625 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose S44625-ANN over S44625-AW?

Pick S44625-ANN when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S44625-ANN and S44625-AW side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.