FabDigitFabDigit

Stainless Steel S32001-CD vs S32001 CW-TR

Stainless Steel · S32001 temper comparison

S32001-CD and S32001 CW-TR are two conditions of the same stainless steel grade, S32001: CD (cold drawn) versus CW-TR (cold Worked / temper rolled strip). The chemistry is identical, so every difference below comes from the condition. Both yield at about 690 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (cold drawn versus cold Worked / temper rolled strip). S32001-CD is the more ductile: elongation 18% versus 14% for S32001 CW-TR. S32001-CD runs hotter in service (300°C vs 250°C continuous).

S32001-CDChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

S32001-CD vs S32001 CW-TR: properties

S32001-CDS32001 CW-TR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

830 MPa120 ksi
850 MPa123 ksi

Yield Strength (0.2% offset)

690 MPa100 ksi
720 MPa104 ksi

Elongation at Break

18%
14%

Reduction in Area

50%
40%

Shear Strength

500 MPa72.5 ksi
510 MPa74 ksi

Fatigue Strength (Endurance Limit)

400 MPa58 ksi
410 MPa59.5 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
80 MPa·√m72.8 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
70 J51.6 ft·lbf

Hardness, Brinell

275 HB
285 HB

Hardness, Rockwell B

104 HRB
103 HRB

Hardness, Rockwell C

28 HRC
29 HRC

Hardness, Vickers

290 HV
300 HV

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.74 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,465°C2,669 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
250°C482 °F

Same in both: Thermal Conductivity 15.5 W/m·K9 BTU/hr·ft·°F · Specific Heat Capacity 480 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 13 µm/m·K7.2 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -50°C-58 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 2.5 % IACS · Electrical Resistivity 7×10⁻⁷ Ω·m27.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

56 / 100
55 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.2 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

38 / 100
35 / 100

Machinability Rating (AISI 1212 = 100 %)

40%
35%

Weldability

65 / 100
60 / 100

Formability (cold)

30 / 100
35 / 100

Same in both: Brazeability / Solderability 35 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 50 MJ/kg21,496 BTU/lb · Embodied Carbon (primary production) 4.5 kg CO₂/kg · Embodied Water 150 L/kg18 gal/lb · Typical Recycled Content 65%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleS32001

S32001-CD vs S32001 CW-TR — frequently asked

What is the difference between S32001-CD and S32001 CW-TR?

S32001-CD and S32001 CW-TR are two conditions of the same stainless steel grade, S32001: CD (cold drawn) versus CW-TR (cold Worked / temper rolled strip). The chemistry is identical, so every difference below comes from the condition. Both yield at about 690 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (cold drawn versus cold Worked / temper rolled strip).

Which condition does FabDigit quote by default, CD or CW-TR?

Annealed is the default S32001 condition in the FabDigit quote flow (neither CD nor CW-TR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, S32001-CD or S32001 CW-TR?

S32001-CD. Its weldability rates good (65/100) against good (60/100) for S32001 CW-TR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S32001-CD and S32001 CW-TR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.