FabDigitFabDigit

ESD-Safe Resin vs Flexible Resin

Polymer · grade comparison

ESD-Safe Resin and Flexible Resin are both polymer grades. ESD-Safe Resin is the stronger of the two: tensile strength 52 MPa (7.54 ksi) against 9 MPa (1.29 ksi) for Flexible Resin, about 5.8 times as much. In exchange, Flexible Resin is the more ductile: elongation 120% versus 6% for ESD-Safe Resin, and ESD-Safe Resin is harder (82 Shore D vs 30 Shore D). Flexible Resin is lighter (1.12 g/cm³ vs 1.17 g/cm³ for ESD-Safe Resin) and ESD-Safe Resin is stiffer (2.4 GPa vs 0.01 GPa). On the shop floor, ESD-Safe Resin machines more easily (good vs poor) and Flexible Resin sits in a lower cost tier (premium, $$$) than ESD-Safe Resin (high, $$$$).

ESD-Safe ResinChoose it when strength drives the design, or when the part is machined in volume.

Flexible ResinChoose it when the part is bent, formed or impact-loaded, or when weight is the constraint.

ESD-Safe Resin vs Flexible Resin: properties

ESD-Safe ResinFlexible Resin

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

2.4 GPa0.35 Msi
0.01 GPa0 Msi

Poisson's Ratio

0.38
0.48

Tensile Strength (Ultimate)

52 MPa7.5 ksi
9 MPa1.3 ksi

Elongation at Break

6%
120%

Compressive Strength

78 MPa11.3 ksi
5 MPa0.65 ksi

Flexural Strength

78 MPa11.3 ksi
—

Flexural Modulus

2.2 GPa0.32 Msi
—

Izod Impact, Notched

22 J/m0.41 ft·lbf/in
—

Hardness, Shore D

82 Shore D
30 Shore D

Hardness, Rockwell M

85 HRM
—

Compressive Modulus

—
0.01 GPa0 Msi

Shear Strength

—
6 MPa0.87 ksi

Hardness, Shore A

—
80 Shore A

Tear Strength

—
24 kN/m137 lbf/in

Compression Set (22 h, 70 °C)

—
4%

Physical

Density and transition temperatures.

Density

1.17 g/cm³0.04 lb/in³
1.12 g/cm³0.04 lb/in³

Glass Transition (Tg)

68°C154 °F
5°C41 °F

Water Absorption (24 h)

0.5%
1.2%

Water Absorption (Saturation)

1.6%
—

Refractive Index

—
1.5

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.22 W/m·K0.13 BTU/hr·ft·°F
0.2 W/m·K0.12 BTU/hr·ft·°F

Specific Heat Capacity

1,450 J/kg·K0.35 BTU/lb·°F
1,650 J/kg·K0.39 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

80 µm/m·K44.4 µin/in·°F
180 µm/m·K100 µin/in·°F

Max Service Temperature (continuous)

60°C140 °F
65°C149 °F

Heat Deflection Temp. @ 0.45 MPa

70°C158 °F
60°C140 °F

Heat Deflection Temp. @ 1.8 MPa

55°C131 °F
—

Limiting Oxygen Index

20%
19%

Max Service Temperature (short-term)

90°C194 °F
85°C185 °F

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1,000,000 Ω·m3.94×10¹³ µΩ·in
1×10¹¹ Ω·m3.94×10¹⁸ µΩ·in

Volume Resistivity

1×10⁸ Ω·cm
1×10¹³ Ω·cm

Surface Resistivity

1×10⁸ Ω
—

Dielectric Strength

—
14 kV/mm356 V/mil

Dielectric Constant (1 MHz)

—
4

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

45 / 100
25 / 100

Same in both: Corrosion Resistance 70 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
15 / 100

Weldability

5 / 100
—

Polishability

40 / 100
25 / 100

Mold Shrinkage

—
1.5%

Same in both: Processing Melt Temperature (typ.) 30°C86 °F

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 115 MJ/kg49,441 BTU/lb · Embodied Carbon (primary production) 5.5 kg CO₂/kg · Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

44 kN·m/kg
8 kN·m/kg

Specific Stiffness (E / density)

2.1 MN·m/kg
0 MN·m/kg

Thermal Shock Resistance Index

0
1

Same in both: Thermal Diffusivity 0.1 mm²/s

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleFlexible Resin

Manufacturing and finishing

CapabilityESD-Safe ResinFlexible Resin
Injection molding—Yes
3D printing—Yes
Default condition—Shore A 80
Relative cost$$$$ High$$$ Premium
Min. machined wall——
Best machined surface——
Chrome Plating (Plastic)—Yes
Conductive Coating—Yes
Dyeing (Nylon)—Yes
EMI Shielding Coating—Yes
Painting—Yes
Primer Coating—Yes
Soft Touch Coating—Yes
Spray Painting—Yes
Tinted Coating—Yes
UV Coating—Yes
Vacuum Metallization—Yes
Waterproof Coating—Yes

ESD-Safe Resin vs Flexible Resin — frequently asked

Is ESD-Safe Resin stronger than Flexible Resin?

Yes. ESD-Safe Resin has a typical tensile strength of 52 MPa (7.54 ksi) against 9 MPa (1.29 ksi) for Flexible Resin — about 5.8 times as much.

Which is cheaper, ESD-Safe Resin or Flexible Resin?

Flexible Resin is the lower-cost material: it sits in the premium tier ($$$) while ESD-Safe Resin is high ($$$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, ESD-Safe Resin or Flexible Resin?

ESD-Safe Resin. Its machinability rates good (55/100) against poor (15/100) for Flexible Resin.

Ready to make it?

Upload a CAD file and FabDigit prices the part in ESD-Safe Resin and Flexible Resin side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.