FabDigitFabDigit

Nickel Alloy Inconel 693 Aged vs Inconel 693-CD

Nickel Alloy · Inconel 693 temper comparison

Inconel 693 Aged and Inconel 693-CD are two conditions of the same nickel alloy grade, Inconel 693: Aged (annealed + Aged) versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. Inconel 693-CD is the stronger of the two: yield strength 700 MPa (102 ksi) against 600 MPa (87 ksi) for Inconel 693 Aged, about 17% more. Inconel 693 Aged is harder — 290 HB against 270 HB for Inconel 693-CD — which matters for wear surfaces and threads. Inconel 693 Aged runs hotter in service (1,100°C vs 600°C continuous).

Inconel 693 AgedChoose it when surface hardness matters, or when the part sees heat.

Inconel 693-CDChoose it when strength drives the design.

Inconel 693 Aged vs Inconel 693-CD: properties

Inconel 693 AgedInconel 693-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
200 GPa29 Msi

Yield Strength (0.2% offset)

600 MPa87 ksi
700 MPa102 ksi

Reduction in Area

32%
35%

Fatigue Strength (Endurance Limit)

380 MPa55.1 ksi
360 MPa52.2 ksi

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
50 J36.9 ft·lbf

Hardness, Brinell

290 HB
270 HB

Same in both: Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 167 GPa24.2 Msi · Poisson's Ratio 0.3 · Tensile Strength (Ultimate) 950 MPa138 ksi · Elongation at Break 25% · Shear Strength 590 MPa85.6 ksi · Hardness, Rockwell B 92 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.63 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,343°C2,449 °F · Liquidus Temperature 1,392°C2,538 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

11 W/m·K6.4 BTU/hr·ft·°F
10.6 W/m·K6.1 BTU/hr·ft·°F

Max Service Temperature (continuous)

1,100°C2,012 °F
600°C1,112 °F

Same in both: Specific Heat Capacity 450 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.6 µm/m·K7 µin/in·°F · Latent Heat of Fusion 290 J/g125 BTU/lb · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

1.5 % IACS
1.4 % IACS

Electrical Resistivity

1.18×10⁻⁶ Ω·m46.5 µΩ·in
1.23×10⁻⁶ Ω·m48.4 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.15 V · Corrosion Resistance 82 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

13 / 100
18 / 100

Machinability Rating (AISI 1212 = 100 %)

8%
13%

Weldability

45 / 100
50 / 100

Formability (cold)

30 / 100
35 / 100

Same in both: Castability 35 / 100 · Brazeability / Solderability 45 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 160 MJ/kg68,788 BTU/lb · Embodied Carbon (primary production) 13 kg CO₂/kg · Embodied Water 500 L/kg59.9 gal/lb · Typical Recycled Content 35%

Strength versus weight

Yield strength against density for every nickel alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0006.577.588.59Density (g/cm³)Yield strength (MPa) — log scaleInconel 693

Inconel 693 Aged vs Inconel 693-CD — frequently asked

Is Inconel 693-CD stronger than Inconel 693 Aged?

Yes. Inconel 693-CD has a typical yield strength of 700 MPa (102 ksi) against 600 MPa (87 ksi) for Inconel 693 Aged — about 17% more. Tensile strength is 950 MPa (138 ksi) vs 950 MPa (138 ksi).

Which condition does FabDigit quote by default, Aged or CD?

ANN is the default Inconel 693 condition in the FabDigit quote flow (neither Aged nor CD). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, Inconel 693 Aged or Inconel 693-CD?

Inconel 693-CD. Its machinability rates poor (18/100) against not recommended (13/100) for Inconel 693 Aged; for welding the order is Inconel 693-CD first (fair, 50/100) then Inconel 693 Aged (fair, 45/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in Inconel 693 Aged and Inconel 693-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.