FabDigitFabDigit

Copper Alloy CC482K-GC vs CC482K-GS

Copper Alloy · CC482K temper comparison

CC482K-GC and CC482K-GS are two conditions of the same copper alloy grade, CC482K: GC (continuous cast bar/tube) versus GS (sand cast). The chemistry is identical, so every difference below comes from the condition. CC482K-GC is the stronger of the two: yield strength 170 MPa (24.7 ksi) against 150 MPa (21.8 ksi) for CC482K-GS, about 13% more; tensile strength follows at 300 MPa (43.5 ksi) vs 270 MPa (39.2 ksi). CC482K-GC is harder — 95 HB against 85 HB for CC482K-GS — which matters for wear surfaces and threads.

CC482K-GCChoose it when strength drives the design, or when surface hardness matters.

CC482K-GC vs CC482K-GS: properties

CC482K-GCCC482K-GS

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

103 GPa14.9 Msi
98 GPa14.2 Msi

Tensile Strength (Ultimate)

300 MPa43.5 ksi
270 MPa39.2 ksi

Yield Strength (0.2% offset)

170 MPa24.7 ksi
150 MPa21.8 ksi

Compressive Strength

560 MPa81.2 ksi
500 MPa72.5 ksi

Shear Strength

218 MPa31.6 ksi
195 MPa28.3 ksi

Fatigue Strength (Endurance Limit)

100 MPa14.5 ksi
90 MPa13.1 ksi

Charpy V-Notch Impact (RT)

11 J8.1 ft·lbf
9 J6.6 ft·lbf

Hardness, Brinell

95 HB
85 HB

Hardness, Rockwell B

55 HRB
45 HRB

Hardness, Vickers

100 HV
90 HV

Same in both: Shear Modulus 39 GPa5.7 Msi · Bulk Modulus 107 GPa15.5 Msi · Poisson's Ratio 0.34 · Elongation at Break 8% · Reduction in Area 10%

Physical

Density and transition temperatures.

Same in both: Density 8.8 g/cm³0.32 lb/in³ · Melting Point (Solidus) 830°C1,526 °F · Liquidus Temperature 990°C1,814 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

47 W/m·K27.2 BTU/hr·ft·°F
45 W/m·K26 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18.5 µm/m·K10.3 µin/in·°F · Latent Heat of Fusion 175 J/g75.2 BTU/lb · Max Service Temperature (continuous) 250°C482 °F · Min Service Temperature -200°C-328 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

11 % IACS
10.5 % IACS

Electrical Resistivity

1.57×10⁻⁷ Ω·m6.18 µΩ·in
1.64×10⁻⁷ Ω·m6.46 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

72 / 100
68 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.31 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
60%

Same in both: Weldability 25 / 100 · Formability (cold) 8 / 100 · Castability 80 / 100 · Brazeability / Solderability 78 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 65 MJ/kg27,945 BTU/lb · Embodied Carbon (primary production) 4.6 kg CO₂/kg · Embodied Water 300 L/kg35.9 gal/lb · Typical Recycled Content 70%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC482K

CC482K-GC vs CC482K-GS — frequently asked

Is CC482K-GC stronger than CC482K-GS?

Yes. CC482K-GC has a typical yield strength of 170 MPa (24.7 ksi) against 150 MPa (21.8 ksi) for CC482K-GS — about 13% more. Tensile strength is 300 MPa (43.5 ksi) vs 270 MPa (39.2 ksi).

Which condition does FabDigit quote by default, GC or GS?

GC is the default CC482K condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC482K-GC over CC482K-GS?

Pick CC482K-GC when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC482K-GC and CC482K-GS side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.