Copper Alloy C94300-M05 vs C94300-M07

Copper Alloy · C94300 temper comparison

C94300-M05 and C94300-M07 are two conditions of the same copper alloy grade, C94300: M05 (as plaster cast) versus M07 (as continuous cast). The chemistry is identical, so every difference below comes from the condition. Both yield at about 100 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as plaster cast versus as continuous cast). C94300-M07 is harder — 55 HB against 52 HB for C94300-M05 — which matters for wear surfaces and threads.

C94300-M07Choose it when surface hardness matters.

C94300-M05 vs C94300-M07: properties

C94300-M05C94300-M07

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

195 MPa28.3 ksi
205 MPa29.7 ksi

Yield Strength (0.2% offset)

100 MPa14.5 ksi
105 MPa15.2 ksi

Shear Strength

138 MPa20 ksi
145 MPa21 ksi

Fatigue Strength (Endurance Limit)

52 MPa7.5 ksi
55 MPa8 ksi

Charpy V-Notch Impact (RT)

12 J8.9 ft·lbf
14 J10.3 ft·lbf

Hardness, Brinell

52 HB
55 HB

Hardness, Vickers

54 HV
57 HV

Same in both: Elastic (Young's) Modulus 72 GPa10.4 Msi · Shear Modulus 27 GPa3.9 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.33 · Elongation at Break 12%

Physical

Density and transition temperatures.

Same in both: Density 9.29 g/cm³0.34 lb/in³ · Melting Point (Solidus) 762°C1,404 °F · Liquidus Temperature 954°C1,749 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 46.7 W/m·K27 BTU/hr·ft·°F · Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18.5 µm/m·K10.3 µin/in·°F · Max Service Temperature (continuous) 230°C446 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 9 % IACS · Electrical Resistivity 1.92×10⁻⁷ Ω·m7.56 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.28 V · Corrosion Resistance 58 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

88 / 100
90 / 100

Same in both: Machinability Rating (AISI 1212 = 100 %) 130% · Weldability 8 / 100 · Formability (cold) 5 / 100 · Castability 85 / 100 · Brazeability / Solderability 35 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 45 MJ/kg19,347 BTU/lb · Embodied Carbon (primary production) 3 kg CO₂/kg · Embodied Water 280 L/kg33.6 gal/lb · Typical Recycled Content 70%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleC94300

C94300-M05 vs C94300-M07 — frequently asked

What is the difference between C94300-M05 and C94300-M07?

C94300-M05 and C94300-M07 are two conditions of the same copper alloy grade, C94300: M05 (as plaster cast) versus M07 (as continuous cast). The chemistry is identical, so every difference below comes from the condition. Both yield at about 100 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as plaster cast versus as continuous cast).

Which condition does FabDigit quote by default, M05 or M07?

M07 is the default C94300 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose C94300-M05 over C94300-M07?

Pick C94300-M07 when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in C94300-M05 and C94300-M07 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.