FabDigitFabDigit

AlN vs TiN

Ceramic · grade comparison

AlN and TiN are both ceramic grades. TiN is harder — 1,900 HV against 1,100 HV for AlN — which matters for wear surfaces and threads. AlN is lighter (3.26 g/cm³ vs 5.22 g/cm³ for TiN) and AlN is stiffer (320 GPa vs 250 GPa).

AlNChoose it when weight is the constraint, or when the part sees heat.

TiNChoose it when surface hardness matters.

AlN vs TiN: properties

AlNTiN

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

320 GPa46.4 Msi
250 GPa36.3 Msi

Shear Modulus

130 GPa18.9 Msi
—

Bulk Modulus

200 GPa29 Msi
290 GPa42.1 Msi

Poisson's Ratio

0.24
0.25

Tensile Strength (Ultimate)

200 MPa29 ksi
—

Compressive Strength

2,100 MPa305 ksi
1,400 MPa203 ksi

Flexural Strength

330 MPa47.9 ksi
350 MPa50.8 ksi

Fracture Toughness (K_IC)

2.7 MPa·√m2.5 ksi·√in
4 MPa·√m3.6 ksi·√in

Hardness, Vickers

1,100 HV
1,900 HV

Hardness, Knoop

1,200 HK
1,800 HK

Hardness, Mohs

7.5
9

Physical

Density and transition temperatures.

Density

3.26 g/cm³0.12 lb/in³
5.22 g/cm³0.19 lb/in³

Melting Point (Solidus)

2,200°C3,992 °F
2,950°C5,342 °F

Refractive Index

2.15
—

Porosity

0.2%
2%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

180 W/m·K104 BTU/hr·ft·°F
29 W/m·K16.8 BTU/hr·ft·°F

Specific Heat Capacity

740 J/kg·K0.18 BTU/lb·°F
600 J/kg·K0.14 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

4.4 µm/m·K2.4 µin/in·°F
9.4 µm/m·K5.2 µin/in·°F

Max Service Temperature (continuous)

900°C1,652 °F
600°C1,112 °F

Min Service Temperature

-200°C-328 °F
-250°C-418 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹² Ω·m3.94×10¹⁹ µΩ·in
3×10⁻⁷ Ω·m11.8 µΩ·in

Dielectric Strength

17 kV/mm432 V/mil
—

Dielectric Constant (1 MHz)

8.8
—

Dissipation Factor (1 MHz)

5×10⁻⁴
—

Volume Resistivity

1×10¹⁴ Ω·cm
3×10⁻⁵ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

85 / 100
75 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

5 / 100
8 / 100

Same in both: Polishability 85 / 100 · Sintering / Firing Temperature 1,800°C3,272 °F

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

280 MJ/kg120,378 BTU/lb
200 MJ/kg85,985 BTU/lb

Embodied Carbon (primary production)

22 kg CO₂/kg
15 kg CO₂/kg

Embodied Water

300 L/kg35.9 gal/lb
—

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Stiffness (E / density)

98.2 MN·m/kg
47.9 MN·m/kg

Thermal Diffusivity

74.6 mm²/s
9.3 mm²/s

Strength versus weight

Yield strength against density for every ceramic grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,000234567Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityAlNTiN
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

AlN vs TiN — frequently asked

What is the difference between AlN and TiN?

AlN and TiN are both ceramic grades. TiN is harder — 1,900 HV against 1,100 HV for AlN — which matters for wear surfaces and threads. AlN is lighter (3.26 g/cm³ vs 5.22 g/cm³ for TiN) and AlN is stiffer (320 GPa vs 250 GPa).

Which is cheaper, AlN or TiN?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose AlN over TiN?

Pick AlN when weight is the constraint, or when the part sees heat. Pick TiN when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in AlN and TiN side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.