Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Tensile Strength (Ultimate)

660 MPa95.7 ksi
670 MPa97.2 ksi
830 MPa120 ksi
965 MPa140 ksi

Yield Strength (0.2% offset)

380 MPa55.1 ksi
380 MPa55.1 ksi
470 MPa68.2 ksi
585 MPa84.8 ksi

Elongation at Break

22%
12%
11%
12%

Reduction in Area

45%
30%
20%
17%

Shear Strength

460 MPa66.7 ksi
430 MPa62.4 ksi
520 MPa75.4 ksi
580 MPa84.1 ksi

Fatigue Strength (Endurance Limit)

285 MPa41.3 ksi
300 MPa43.5 ksi
370 MPa53.7 ksi
420 MPa60.9 ksi

Charpy V-Notch Impact (RT)

28 J20.7 ft·lbf
10 J7.4 ft·lbf
9 J6.6 ft·lbf
8 J5.9 ft·lbf

Hardness, Brinell

190 HB
190 HB
235 HB
293 HB

Hardness, Rockwell B

91 HRB
92 HRB
99 HRB

Compressive Strength

380 MPa55.1 ksi

Fracture Toughness (K_IC)

45 MPa·√m41 ksi·√in

Hardness, Vickers

247 HV

Hardness, Rockwell C

31 HRC

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,420°C2,588 °F
1,425°C2,597 °F
1,425°C2,597 °F
1,425°C2,597 °F

Liquidus Temperature

1,470°C2,678 °F
1,480°C2,696 °F
1,470°C2,678 °F
1,470°C2,678 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

48 W/m·K27.7 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F
48 W/m·K27.7 BTU/hr·ft·°F
48 W/m·K27.7 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.7 µm/m·K6.5 µin/in·°F
11.3 µm/m·K6.3 µin/in·°F
11.5 µm/m·K6.4 µin/in·°F
11.3 µm/m·K6.3 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
247 J/g106 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

400°C752 °F
350°C662 °F
300°C572 °F
400°C752 °F

Min Service Temperature

-20°C-4 °F
-20°C-4 °F
-30°C-22 °F
-20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

10 % IACS
9.5 % IACS
9.5 % IACS
9.6 % IACS

Electrical Resistivity

1.7×10⁻⁷ Ω·m6.69 µΩ·in
1.8×10⁻⁷ Ω·m7.09 µΩ·in
1.8×10⁻⁷ Ω·m7.09 µΩ·in
1.8×10⁻⁷ Ω·m7.09 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.65 V
-0.61 V

Corrosion Resistance

10 / 100
10 / 100
8 / 100
8 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
45 / 100
38 / 100
35 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
57%
40%
45%

Weldability

20 / 100
25 / 100
18 / 100
20 / 100

Formability (cold)

45 / 100
30 / 100
35 / 100
30 / 100

Castability

45 / 100
45 / 100
40 / 100

Brazeability / Solderability

55 / 100
55 / 100
45 / 100
60 / 100

Polishability

60 / 100
65 / 100
70 / 100
75 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

26 MJ/kg11,178 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2.1 kg CO₂/kg
1.9 kg CO₂/kg
1.9 kg CO₂/kg
1.9 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
30 L/kg3.6 gal/lb
40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

25%
30%
28%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

84 kN·m/kg
85 kN·m/kg
106 kN·m/kg
123 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

344 kJ/m³
352 kJ/m³
539 kJ/m³
835 kJ/m³

Thermal Diffusivity

13 mm²/s
13.3 mm²/s
12.9 mm²/s
13 mm²/s

Thermal Shock Resistance Index

13
14
17
20

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale10651075108460#

Manufacturing and finishing

Capability60#106510751084
Default conditionAnnealedHRHRHR
Relative cost$$ Standard$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 60# and 1065 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.