30NiCrMo16 vs 40CrNiMoA and 2 more: properties

30NiCrMo1640CrNiMoAH1118Ni(200) Maraging Steel

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
207 GPa30 Msi
210 GPa30.5 Msi
186 GPa27 Msi

Shear Modulus

80 GPa11.6 Msi
80 GPa11.6 Msi
81 GPa11.7 Msi
71 GPa10.3 Msi

Poisson's Ratio

0.29
0.29
0.29
0.3

Tensile Strength (Ultimate)

1,860 MPa270 ksi
1,080 MPa157 ksi
800 MPa116 ksi
1,450 MPa210 ksi

Yield Strength (0.2% offset)

1,620 MPa235 ksi
950 MPa138 ksi
510 MPa74 ksi
1,400 MPa203 ksi

Elongation at Break

12%
16%
20%
12%

Reduction in Area

48%
58%
45%
60%

Compressive Strength

1,680 MPa244 ksi
980 MPa142 ksi
1,420 MPa206 ksi

Shear Strength

1,120 MPa162 ksi
660 MPa95.7 ksi
500 MPa72.5 ksi
870 MPa126 ksi

Fatigue Strength (Endurance Limit)

780 MPa113 ksi
520 MPa75.4 ksi
600 MPa87 ksi

Fracture Toughness (K_IC)

80 MPa·√m72.8 ksi·√in
90 MPa·√m81.9 ksi·√in
155 MPa·√m141 ksi·√in

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
70 J51.6 ft·lbf
40 J29.5 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

520 HB
320 HB
200 HB
400 HB

Hardness, Rockwell C

53 HRC
34 HRC
43 HRC

Hardness, Vickers

560 HV
335 HV
210 HV
420 HV

Hardness, Rockwell B

94 HRB

Same in both: Bulk Modulus 160 GPa23.2 Msi

Physical

Density and transition temperatures.

Density

7.85 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.8 g/cm³0.28 lb/in³
8 g/cm³0.29 lb/in³

Melting Point (Solidus)

1,420°C2,588 °F
1,420°C2,588 °F
1,427°C2,601 °F
1,413°C2,575 °F

Liquidus Temperature

1,490°C2,714 °F
1,500°C2,732 °F
1,470°C2,678 °F
1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

33 W/m·K19.1 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
25 W/m·K14.4 BTU/hr·ft·°F
20.5 W/m·K11.8 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
452 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.8 µm/m·K6.6 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
10.1 µm/m·K5.6 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
540°C1,004 °F
400°C752 °F

Min Service Temperature

-70°C-94 °F
-60°C-76 °F
-40°C-40 °F
-196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

6.8 % IACS
7 % IACS
3.3 % IACS
3.8 % IACS

Electrical Resistivity

2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.48×10⁻⁷ Ω·m9.76 µΩ·in
5.2×10⁻⁷ Ω·m20.5 µΩ·in
4.5×10⁻⁷ Ω·m17.7 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.6 V
-0.6 V
-0.52 V

Corrosion Resistance

14 / 100
15 / 100
18 / 100
25 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

15 / 100
42 / 100
55 / 100
30 / 100

Machinability Rating (AISI 1212 = 100 %)

10%
45%
45%
30%

Weldability

15 / 100
30 / 100
35 / 100
70 / 100

Formability (cold)

8 / 100
25 / 100
30 / 100
15 / 100

Brazeability / Solderability

35 / 100
45 / 100
40 / 100
50 / 100

Polishability

75 / 100
65 / 100
75 / 100
80 / 100

Castability

40 / 100
30 / 100
45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

36 MJ/kg15,477 BTU/lb
32 MJ/kg13,758 BTU/lb
34 MJ/kg14,617 BTU/lb
110 MJ/kg47,292 BTU/lb

Embodied Carbon (primary production)

2.6 kg CO₂/kg
2.3 kg CO₂/kg
2.5 kg CO₂/kg
7.5 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
55 L/kg6.6 gal/lb
70 L/kg8.4 gal/lb
200 L/kg24 gal/lb

Typical Recycled Content

30%
30%
40%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

237 kN·m/kg
138 kN·m/kg
103 kN·m/kg
181 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
26.4 MN·m/kg
26.9 MN·m/kg
23.3 MN·m/kg

Modulus of Resilience

6,401 kJ/m³
2,180 kJ/m³
619 kJ/m³
5,269 kJ/m³

Thermal Diffusivity

8.9 mm²/s
11.8 mm²/s
7 mm²/s
5.7 mm²/s

Thermal Shock Resistance Index

25
19
8
16

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale40CrNiMoAH1118Ni(200) Maraging Steel30NiCrMo16

Manufacturing and finishing

Capability30NiCrMo1640CrNiMoAH1118Ni(200) Maraging Steel
CNC machiningYesYes
Sheet metalYes
Default conditionQ&TAnnealed
Relative cost$$$ Premium$$ Standard$$ Standard$$$$ High
Min. machined wall0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µm
AlCrNYesYes
AlTiNYesYes
Black OxideYesYes
CVD Al2O3YesYes
CVD TiCNYesYes
CVD TiNYesYes
CerakoteYesYes
Chrome PlatingYesYes
CrNYesYes
DLCYesYes
E-CoatingYesYes
HVOF CoatingYesYes
Hot-Dip GalvanizingYesYes
MoS2YesYes
Multilayer CVDYesYes
Nickel PlatingYesYes
PTFE CoatingYesYes
PaintingYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 30NiCrMo16 and 40CrNiMoA side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.