Elastic (Young's) Modulus

70.3 GPa10.2 Msi
69 GPa10 Msi
73 GPa10.6 Msi
71 GPa10.3 Msi

Shear Modulus

26.4 GPa3.8 Msi
26 GPa3.8 Msi
27 GPa3.9 Msi
26.4 GPa3.8 Msi

Bulk Modulus

68 GPa9.9 Msi
76 GPa11 Msi
75 GPa10.9 Msi
70 GPa10.2 Msi

Tensile Strength (Ultimate)

240 MPa34.8 ksi
125 MPa18.1 ksi
200 MPa29 ksi
300 MPa43.5 ksi

Yield Strength (0.2% offset)

115 MPa16.7 ksi
115 MPa16.7 ksi
110 MPa16 ksi
145 MPa21 ksi

Elongation at Break

20%
12%
16%
20%

Shear Strength

145 MPa21 ksi
75 MPa10.9 ksi
130 MPa18.9 ksi
175 MPa25.4 ksi

Fatigue Strength (Endurance Limit)

110 MPa16 ksi
48 MPa7 ksi
70 MPa10.2 ksi
145 MPa21 ksi

Hardness, Brinell

58 HB
32 HB
60 HB
80 HB

Hardness, Vickers

35 HV

Fracture Toughness (K_IC)

32 MPa·√m29.1 ksi·√in
28 MPa·√m25.5 ksi·√in

Same in both: Poisson's Ratio 0.33

Physical

Density and transition temperatures.

Density

2.66 g/cm³0.1 lb/in³
2.71 g/cm³0.1 lb/in³
2.84 g/cm³0.1 lb/in³
2.66 g/cm³0.1 lb/in³

Melting Point (Solidus)

593°C1,099 °F
643°C1,189 °F
543°C1,009 °F
574°C1,065 °F

Liquidus Temperature

643°C1,189 °F
657°C1,215 °F
643°C1,189 °F
638°C1,180 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

127 W/m·K73.4 BTU/hr·ft·°F
222 W/m·K128 BTU/hr·ft·°F
170 W/m·K98.2 BTU/hr·ft·°F
117 W/m·K67.6 BTU/hr·ft·°F

Specific Heat Capacity

900 J/kg·K0.21 BTU/lb·°F
904 J/kg·K0.22 BTU/lb·°F
864 J/kg·K0.21 BTU/lb·°F
900 J/kg·K0.21 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

23.9 µm/m·K13.3 µin/in·°F
23.6 µm/m·K13.1 µin/in·°F
22.3 µm/m·K12.4 µin/in·°F
23.4 µm/m·K13 µin/in·°F

Latent Heat of Fusion

390 J/g168 BTU/lb
397 J/g171 BTU/lb
385 J/g166 BTU/lb
397 J/g171 BTU/lb

Max Service Temperature (continuous)

65°C149 °F
120°C248 °F
175°C347 °F
65°C149 °F

Min Service Temperature

-196°C-321 °F
-273°C-459 °F
-253°C-423 °F
-270°C-454 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

33 % IACS
57 % IACS
44 % IACS
29 % IACS

Electrical Resistivity

5.2×10⁻⁸ Ω·m2.05 µΩ·in
3.02×10⁻⁸ Ω·m1.19 µΩ·in
3.9×10⁻⁸ Ω·m1.54 µΩ·in
5.9×10⁻⁸ Ω·m2.32 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.87 V
-0.83 V
-0.64 V
-0.87 V

Corrosion Resistance

80 / 100
78 / 100
32 / 100
75 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
38 / 100
62 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
30%
55%
45%

Weldability

92 / 100
95 / 100
92 / 100
95 / 100

Formability (cold)

80 / 100
85 / 100
55 / 100
70 / 100

Brazeability / Solderability

15 / 100
92 / 100
20 / 100
15 / 100

Polishability

55 / 100
80 / 100
55 / 100
60 / 100

Castability

30 / 100
60 / 100
25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

200 MJ/kg85,985 BTU/lb
210 MJ/kg90,284 BTU/lb
205 MJ/kg88,134 BTU/lb
200 MJ/kg85,985 BTU/lb

Embodied Water

1,200 L/kg144 gal/lb
1,200 L/kg144 gal/lb
1,150 L/kg138 gal/lb
1,200 L/kg144 gal/lb

Typical Recycled Content

5%
25%
10%
30%

Same in both: Embodied Carbon (primary production) 12.5 kg CO₂/kg

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

90 kN·m/kg
46 kN·m/kg
70 kN·m/kg
113 kN·m/kg

Specific Stiffness (E / density)

26.4 MN·m/kg
25.5 MN·m/kg
25.7 MN·m/kg
26.7 MN·m/kg

Modulus of Resilience

94 kJ/m³
96 kJ/m³
83 kJ/m³
148 kJ/m³

Thermal Diffusivity

53 mm²/s
90.6 mm²/s
69.3 mm²/s
48.9 mm²/s

Thermal Shock Resistance Index

18
17
21
21

Strength versus weight

Yield strength against density for every aluminum grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

20501002005002.22.42.62.83Density (g/cm³)Yield strength (MPa) — log scale110023195183ER5654

Manufacturing and finishing

CapabilityER5654110023195183
CNC machiningYesYesYes
Sheet metalYesYesYes
Default condition
Relative cost$$$$ High$ Budget$$$ Premium$$ Standard
Min. machined wall0.5 mm0.5 mm0.5 mm
Best machined surfaceRa 0.8 µmRa 0.8 µmRa 0.8 µm
Anodizing Type IIYesYesYes
CerakoteYesYesYes
Chem Film (Alodine)YesYesYes
DLCYesYesYes
E-CoatingYesYesYes
ElectropolishingYesYesYes
Hard Anodize Type III w/ PTFEYesYesYes
Hard Anodizing Type IIIYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes
Powder CoatingYesYesYes

They share 4 finishes: Electroless Nickel (EN), Epoxy Coating, Gold Plating, Silver Plating.

Ready to make it?

Upload a CAD file and FabDigit prices the part in ER5654 and 1100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.