BT5-1-AW and BT5-1-SR are two conditions of the same titanium grade, BT5-1: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 800 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as-welded deposit versus stress relieved). BT5-1-SR is the more ductile: elongation 12% versus 8% for BT5-1-AW.

BT5-1-SRChoose it when the part is bent, formed or impact-loaded.

BT5-1-AW vs BT5-1-SR: properties

BT5-1-AWBT5-1-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

850 MPa123 ksi
880 MPa128 ksi

Yield Strength (0.2% offset)

800 MPa116 ksi
820 MPa119 ksi

Elongation at Break

8%
12%

Reduction in Area

18%
28%

Compressive Strength

830 MPa120 ksi
850 MPa123 ksi

Shear Strength

545 MPa79 ksi
565 MPa81.9 ksi

Fatigue Strength (Endurance Limit)

380 MPa55.1 ksi
510 MPa74 ksi

Fracture Toughness (K_IC)

45 MPa·√m41 ksi·√in
58 MPa·√m52.8 ksi·√in

Charpy V-Notch Impact (RT)

18 J13.3 ft·lbf
22 J16.2 ft·lbf

Hardness, Brinell

315 HB
310 HB

Hardness, Vickers

330 HV
325 HV

Same in both: Elastic (Young's) Modulus 110 GPa16 Msi · Shear Modulus 43 GPa6.2 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.31 · Hardness, Rockwell C 33 HRC

Physical

Density and transition temperatures.

Same in both: Density 4.46 g/cm³0.16 lb/in³ · Melting Point (Solidus) 1,550°C2,822 °F · Liquidus Temperature 1,600°C2,912 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

425°C797 °F
450°C842 °F

Same in both: Thermal Conductivity 7.8 W/m·K4.5 BTU/hr·ft·°F · Specific Heat Capacity 500 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 9.4 µm/m·K5.2 µin/in·°F · Latent Heat of Fusion 390 J/g168 BTU/lb · Min Service Temperature -253°C-423 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 1.1 % IACS · Electrical Resistivity 1.57×10⁻⁶ Ω·m61.8 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

82 / 100
85 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

20 / 100
21 / 100

Machinability Rating (AISI 1212 = 100 %)

20%
21%

Weldability

70 / 100
75 / 100

Formability (cold)

20 / 100
32 / 100

Same in both: Castability 40 / 100 · Brazeability / Solderability 45 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 650 MJ/kg279,450 BTU/lb · Embodied Carbon (primary production) 40 kg CO₂/kg · Embodied Water 500 L/kg59.9 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every titanium grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0004.555.5Density (g/cm³)Yield strength (MPa) — log scaleBT5-1

BT5-1-AW vs BT5-1-SR — frequently asked

What is the difference between BT5-1-AW and BT5-1-SR?

BT5-1-AW and BT5-1-SR are two conditions of the same titanium grade, BT5-1: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 800 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as-welded deposit versus stress relieved).

Which condition does FabDigit quote by default, AW or SR?

Annealed is the default BT5-1 condition in the FabDigit quote flow (neither AW nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, BT5-1-AW or BT5-1-SR?

BT5-1-SR. Its weldability rates very good (75/100) against very good (70/100) for BT5-1-AW.