Steel SUJ4-CD vs SUJ4-HR

Steel · SUJ4 temper comparison

SUJ4-CD and SUJ4-HR are two conditions of the same steel grade, SUJ4: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. SUJ4-CD is the stronger of the two: yield strength 620 MPa (89.9 ksi) against 550 MPa (79.8 ksi) for SUJ4-HR, about 13% more. SUJ4-HR is harder — 270 HB against 235 HB for SUJ4-CD — which matters for wear surfaces and threads. On the shop floor, SUJ4-CD machines more easily (fair vs poor).

SUJ4-CDChoose it when strength drives the design, or when the part is machined in volume.

SUJ4-HRChoose it when surface hardness matters.

SUJ4-CD vs SUJ4-HR: properties

SUJ4-CDSUJ4-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

800 MPa116 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

620 MPa89.9 ksi
550 MPa79.8 ksi

Reduction in Area

38%
30%

Compressive Strength

640 MPa92.8 ksi
570 MPa82.7 ksi

Shear Strength

480 MPa69.6 ksi
570 MPa82.7 ksi

Fatigue Strength (Endurance Limit)

370 MPa53.7 ksi
420 MPa60.9 ksi

Charpy V-Notch Impact (RT)

14 J10.3 ft·lbf
10 J7.4 ft·lbf

Hardness, Brinell

235 HB
270 HB

Hardness, Rockwell B

99 HRB
91 HRB

Hardness, Vickers

248 HV
285 HV

Same in both: Elastic (Young's) Modulus 208 GPa30.2 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Elongation at Break 12%

Physical

Density and transition temperatures.

Same in both: Density 7.81 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,400°C2,552 °F · Liquidus Temperature 1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 465 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -50°C-58 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 3.5 % IACS · Electrical Resistivity 5×10⁻⁷ Ω·m19.7 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
25 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
25%

Formability (cold)

20 / 100
15 / 100

Same in both: Weldability 8 / 100 · Brazeability / Solderability 35 / 100 · Polishability 85 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 33 MJ/kg14,187 BTU/lb · Embodied Carbon (primary production) 2.4 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSUJ4

SUJ4-CD vs SUJ4-HR — frequently asked

Is SUJ4-CD stronger than SUJ4-HR?

Yes. SUJ4-CD has a typical yield strength of 620 MPa (89.9 ksi) against 550 MPa (79.8 ksi) for SUJ4-HR — about 13% more. Tensile strength is 800 MPa (116 ksi) vs 950 MPa (138 ksi).

Which condition does FabDigit quote by default, CD or HR?

A is the default SUJ4 condition in the FabDigit quote flow (neither CD nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SUJ4-CD or SUJ4-HR?

SUJ4-CD. Its machinability rates fair (45/100) against poor (25/100) for SUJ4-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SUJ4-CD and SUJ4-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.