FabDigitFabDigit

Steel SNCM431-CD vs SNCM431-HR

Steel · SNCM431 temper comparison

SNCM431-CD and SNCM431-HR are two conditions of the same steel grade, SNCM431: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. SNCM431-CD is the stronger of the two: yield strength 650 MPa (94.3 ksi) against 520 MPa (75.4 ksi) for SNCM431-HR, about 25% more. In exchange, SNCM431-HR is the more ductile: elongation 19% versus 12% for SNCM431-CD. SNCM431-HR runs hotter in service (400°C vs 350°C continuous).

SNCM431-CDChoose it when strength drives the design.

SNCM431-HRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

SNCM431-CD vs SNCM431-HR: properties

SNCM431-CDSNCM431-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

780 MPa113 ksi
800 MPa116 ksi

Yield Strength (0.2% offset)

650 MPa94.3 ksi
520 MPa75.4 ksi

Elongation at Break

12%
19%

Reduction in Area

40%
45%

Compressive Strength

670 MPa97.2 ksi
540 MPa78.3 ksi

Shear Strength

485 MPa70.3 ksi
495 MPa71.8 ksi

Fatigue Strength (Endurance Limit)

350 MPa50.8 ksi
360 MPa52.2 ksi

Fracture Toughness (K_IC)

95 MPa·√m86.5 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

30 J22.1 ft·lbf
42 J31 ft·lbf

Hardness, Brinell

230 HB
235 HB

Hardness, Rockwell C

20 HRC
21 HRC

Hardness, Vickers

242 HV
247 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F

Same in both: Thermal Conductivity 44 W/m·K25.4 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.15×10⁻⁷ Ω·m8.46 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
54 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
58%

Weldability

40 / 100
45 / 100

Formability (cold)

25 / 100
35 / 100

Same in both: Castability 25 / 100 · Brazeability / Solderability 55 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSNCM431

SNCM431-CD vs SNCM431-HR — frequently asked

Is SNCM431-CD stronger than SNCM431-HR?

Yes. SNCM431-CD has a typical yield strength of 650 MPa (94.3 ksi) against 520 MPa (75.4 ksi) for SNCM431-HR — about 25% more. Tensile strength is 780 MPa (113 ksi) vs 800 MPa (116 ksi).

Which condition does FabDigit quote by default, CD or HR?

QT is the default SNCM431 condition in the FabDigit quote flow (neither CD nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SNCM431-CD or SNCM431-HR?

SNCM431-CD. Its machinability rates good (60/100) against fair (54/100) for SNCM431-HR; for welding the order is SNCM431-HR first (fair, 45/100) then SNCM431-CD (fair, 40/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in SNCM431-CD and SNCM431-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.