FabDigitFabDigit

Steel SNCM431-A vs SNCM431-HR

Steel · SNCM431 temper comparison

SNCM431-A and SNCM431-HR are two conditions of the same steel grade, SNCM431: A (solution annealed) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. SNCM431-HR is the stronger of the two: yield strength 520 MPa (75.4 ksi) against 470 MPa (68.2 ksi) for SNCM431-A, about 11% more; tensile strength follows at 800 MPa (116 ksi) vs 690 MPa (100 ksi). In exchange, SNCM431-A is the more ductile: elongation 23% versus 19% for SNCM431-HR, and SNCM431-HR is harder (235 HB vs 200 HB).

SNCM431-AChoose it when the part is bent, formed or impact-loaded.

SNCM431-HRChoose it when strength drives the design.

SNCM431-A vs SNCM431-HR: properties

SNCM431-ASNCM431-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

690 MPa100 ksi
800 MPa116 ksi

Yield Strength (0.2% offset)

470 MPa68.2 ksi
520 MPa75.4 ksi

Elongation at Break

23%
19%

Reduction in Area

55%
45%

Compressive Strength

780 MPa113 ksi
540 MPa78.3 ksi

Shear Strength

560 MPa81.2 ksi
495 MPa71.8 ksi

Fatigue Strength (Endurance Limit)

320 MPa46.4 ksi
360 MPa52.2 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
42 J31 ft·lbf

Hardness, Brinell

200 HB
235 HB

Hardness, Rockwell C

28 HRC
21 HRC

Hardness, Vickers

290 HV
247 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

42 W/m·K24.3 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

7.8 % IACS
8 % IACS

Electrical Resistivity

2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.15×10⁻⁷ Ω·m8.46 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
54 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
58%

Formability (cold)

45 / 100
35 / 100

Same in both: Weldability 45 / 100 · Castability 25 / 100 · Brazeability / Solderability 55 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSNCM431

SNCM431-A vs SNCM431-HR — frequently asked

Is SNCM431-HR stronger than SNCM431-A?

Yes. SNCM431-HR has a typical yield strength of 520 MPa (75.4 ksi) against 470 MPa (68.2 ksi) for SNCM431-A — about 11% more. Tensile strength is 800 MPa (116 ksi) vs 690 MPa (100 ksi).

Which condition does FabDigit quote by default, A or HR?

QT is the default SNCM431 condition in the FabDigit quote flow (neither A nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SNCM431-A or SNCM431-HR?

SNCM431-A. Its machinability rates good (60/100) against fair (54/100) for SNCM431-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SNCM431-A and SNCM431-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.