SM400A-SR and SM400A TMCP are two conditions of the same steel grade, SM400A: SR (stress relieved) versus TMCP (thermomechanically controlled processed). The chemistry is identical, so every difference below comes from the condition. SM400A TMCP is the stronger of the two: yield strength 305 MPa (44.2 ksi) against 260 MPa (37.7 ksi) for SM400A-SR, about 17% more; tensile strength follows at 460 MPa (66.7 ksi) vs 425 MPa (61.6 ksi). SM400A TMCP is harder — 135 HB against 115 HB for SM400A-SR — which matters for wear surfaces and threads.

SM400A TMCPChoose it when strength drives the design, or when surface hardness matters.

SM400A-SR vs SM400A TMCP: properties

SM400A-SRSM400A TMCP

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

425 MPa61.6 ksi
460 MPa66.7 ksi

Yield Strength (0.2% offset)

260 MPa37.7 ksi
305 MPa44.2 ksi

Elongation at Break

30%
28%

Reduction in Area

55%
53%

Compressive Strength

260 MPa37.7 ksi
305 MPa44.2 ksi

Shear Strength

265 MPa38.4 ksi
290 MPa42.1 ksi

Fatigue Strength (Endurance Limit)

190 MPa27.6 ksi
220 MPa31.9 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

50 J36.9 ft·lbf
100 J73.8 ft·lbf

Hardness, Brinell

115 HB
135 HB

Hardness, Rockwell B

65 HRB
74 HRB

Hardness, Vickers

121 HV
142 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

52 W/m·K30 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Min Service Temperature

0°C32 °F
-20°C-4 °F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 350°C662 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

11 % IACS
10.8 % IACS

Electrical Resistivity

1.57×10⁻⁷ Ω·m6.18 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

68 / 100
62 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
68%

Weldability

95 / 100
97 / 100

Formability (cold)

86 / 100
80 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSM400A

SM400A-SR vs SM400A TMCP — frequently asked

Is SM400A TMCP stronger than SM400A-SR?

Yes. SM400A TMCP has a typical yield strength of 305 MPa (44.2 ksi) against 260 MPa (37.7 ksi) for SM400A-SR — about 17% more. Tensile strength is 460 MPa (66.7 ksi) vs 425 MPa (61.6 ksi).

Which condition does FabDigit quote by default, SR or TMCP?

HR is the default SM400A condition in the FabDigit quote flow (neither SR nor TMCP). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SM400A-SR or SM400A TMCP?

SM400A-SR, by a small margin. Both rate good for machinability — 68/100 against 62/100 for SM400A TMCP.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SM400A-SR and SM400A TMCP side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.