SCM432-CD and SCM432-N are two conditions of the same steel grade, SCM432: CD (cold drawn) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. SCM432-CD is the stronger of the two: yield strength 650 MPa (94.3 ksi) against 470 MPa (68.2 ksi) for SCM432-N, about 38% more; tensile strength follows at 780 MPa (113 ksi) vs 740 MPa (107 ksi). In exchange, SCM432-N is the more ductile: elongation 20% versus 12% for SCM432-CD, and SCM432-CD is harder (229 HB vs 217 HB). SCM432-N runs hotter in service (400°C vs 300°C continuous).

SCM432-CDChoose it when strength drives the design.

SCM432-NChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

SCM432-CD vs SCM432-N: properties

SCM432-CDSCM432-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

780 MPa113 ksi
740 MPa107 ksi

Yield Strength (0.2% offset)

650 MPa94.3 ksi
470 MPa68.2 ksi

Elongation at Break

12%
20%

Reduction in Area

40%
52%

Compressive Strength

660 MPa95.7 ksi
480 MPa69.6 ksi

Shear Strength

470 MPa68.2 ksi
445 MPa64.5 ksi

Fatigue Strength (Endurance Limit)

370 MPa53.7 ksi
350 MPa50.8 ksi

Fracture Toughness (K_IC)

65 MPa·√m59.2 ksi·√in
75 MPa·√m68.3 ksi·√in

Charpy V-Notch Impact (RT)

28 J20.7 ft·lbf
50 J36.9 ft·lbf

Hardness, Brinell

229 HB
217 HB

Hardness, Rockwell C

20 HRC
17 HRC

Hardness, Vickers

241 HV
228 HV

Same in both: Elastic (Young's) Modulus 207 GPa30 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

43 W/m·K24.8 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Max Service Temperature (continuous)

300°C572 °F
400°C752 °F

Same in both: Specific Heat Capacity 473 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8 % IACS
8.2 % IACS

Electrical Resistivity

2.15×10⁻⁷ Ω·m8.46 µΩ·in
2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
60 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
60%

Weldability

42 / 100
50 / 100

Formability (cold)

30 / 100
48 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 28 MJ/kg12,038 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM432

SCM432-CD vs SCM432-N — frequently asked

Is SCM432-CD stronger than SCM432-N?

Yes. SCM432-CD has a typical yield strength of 650 MPa (94.3 ksi) against 470 MPa (68.2 ksi) for SCM432-N — about 38% more. Tensile strength is 780 MPa (113 ksi) vs 740 MPa (107 ksi).

Which condition does FabDigit quote by default, CD or N?

QT is the default SCM432 condition in the FabDigit quote flow (neither CD nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, SCM432-CD or SCM432-N?

SCM432-N. Its weldability rates fair (50/100) against fair (42/100) for SCM432-CD.