FabDigitFabDigit

Steel SCM421-HR vs SCM421-N

Steel · SCM421 temper comparison

SCM421-HR and SCM421-N are two conditions of the same steel grade, SCM421: HR (hot rolled) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. SCM421-N is the stronger of the two: yield strength 460 MPa (66.7 ksi) against 430 MPa (62.4 ksi) for SCM421-HR, about 7% more; tensile strength follows at 720 MPa (104 ksi) vs 680 MPa (98.6 ksi).

SCM421-NChoose it when strength drives the design.

SCM421-HR vs SCM421-N: properties

SCM421-HRSCM421-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

680 MPa98.6 ksi
720 MPa104 ksi

Yield Strength (0.2% offset)

430 MPa62.4 ksi
460 MPa66.7 ksi

Reduction in Area

48%
50%

Shear Strength

415 MPa60.2 ksi
440 MPa63.8 ksi

Fatigue Strength (Endurance Limit)

300 MPa43.5 ksi
320 MPa46.4 ksi

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
55 J40.6 ft·lbf

Hardness, Brinell

200 HB
210 HB

Hardness, Rockwell B

93 HRB
95 HRB

Same in both: Elastic (Young's) Modulus 206 GPa29.9 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Elongation at Break 20%

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 42 W/m·K24.3 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Formability (cold)

45 / 100
42 / 100

Same in both: Machinability 57 / 100 · Machinability Rating (AISI 1212 = 100 %) 55% · Weldability 45 / 100 · Brazeability / Solderability 60 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM421

SCM421-HR vs SCM421-N — frequently asked

Is SCM421-N stronger than SCM421-HR?

Yes. SCM421-N has a typical yield strength of 460 MPa (66.7 ksi) against 430 MPa (62.4 ksi) for SCM421-HR — about 7% more. Tensile strength is 720 MPa (104 ksi) vs 680 MPa (98.6 ksi).

Which condition does FabDigit quote by default, HR or N?

A is the default SCM421 condition in the FabDigit quote flow (neither HR nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose SCM421-HR over SCM421-N?

Pick SCM421-N when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SCM421-HR and SCM421-N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.