Steel SCM421-CD vs SCM421-HR

Steel · SCM421 temper comparison

SCM421-CD and SCM421-HR are two conditions of the same steel grade, SCM421: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. SCM421-CD is the stronger of the two: yield strength 590 MPa (85.6 ksi) against 430 MPa (62.4 ksi) for SCM421-HR, about 37% more. In exchange, SCM421-HR is the more ductile: elongation 20% versus 12% for SCM421-CD. On the shop floor, SCM421-CD machines more easily (67 vs 57 out of 100).

SCM421-CDChoose it when strength drives the design, or when the part is machined in volume.

SCM421-HRChoose it when the part is bent, formed or impact-loaded.

SCM421-CD vs SCM421-HR: properties

SCM421-CDSCM421-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

700 MPa102 ksi
680 MPa98.6 ksi

Yield Strength (0.2% offset)

590 MPa85.6 ksi
430 MPa62.4 ksi

Elongation at Break

12%
20%

Reduction in Area

40%
48%

Shear Strength

425 MPa61.6 ksi
415 MPa60.2 ksi

Fatigue Strength (Endurance Limit)

310 MPa45 ksi
300 MPa43.5 ksi

Charpy V-Notch Impact (RT)

35 J25.8 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

210 HB
200 HB

Hardness, Rockwell B

95 HRB
93 HRB

Same in both: Elastic (Young's) Modulus 206 GPa29.9 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 42 W/m·K24.3 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

67 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
55%

Weldability

42 / 100
45 / 100

Formability (cold)

30 / 100
45 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM421

SCM421-CD vs SCM421-HR — frequently asked

Is SCM421-CD stronger than SCM421-HR?

Yes. SCM421-CD has a typical yield strength of 590 MPa (85.6 ksi) against 430 MPa (62.4 ksi) for SCM421-HR — about 37% more. Tensile strength is 700 MPa (102 ksi) vs 680 MPa (98.6 ksi).

Which condition does FabDigit quote by default, CD or HR?

A is the default SCM421 condition in the FabDigit quote flow (neither CD nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SCM421-CD or SCM421-HR?

SCM421-CD, by a small margin. Both rate good for machinability — 67/100 against 57/100 for SCM421-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SCM421-CD and SCM421-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.