FabDigitFabDigit

Steel SCM420-CD vs SCM420-CR

Steel · SCM420 temper comparison

SCM420-CD and SCM420-CR are two conditions of the same steel grade, SCM420: CD (cold drawn) versus CR (cold rolled). The chemistry is identical, so every difference below comes from the condition. SCM420-CD is the stronger of the two: yield strength 620 MPa (89.9 ksi) against 580 MPa (84.1 ksi) for SCM420-CR, about 7% more; tensile strength follows at 760 MPa (110 ksi) vs 720 MPa (104 ksi).

SCM420-CDChoose it when strength drives the design.

SCM420-CD vs SCM420-CR: properties

SCM420-CDSCM420-CR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

760 MPa110 ksi
720 MPa104 ksi

Yield Strength (0.2% offset)

620 MPa89.9 ksi
580 MPa84.1 ksi

Elongation at Break

13%
14%

Reduction in Area

42%
40%

Shear Strength

460 MPa66.7 ksi
440 MPa63.8 ksi

Fatigue Strength (Endurance Limit)

340 MPa49.3 ksi
325 MPa47.1 ksi

Charpy V-Notch Impact (RT)

28 J20.7 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

225 HB
215 HB

Hardness, Rockwell B

97 HRB
95 HRB

Same in both: Elastic (Young's) Modulus 207 GPa30 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Fracture Toughness (K_IC) 60 MPa·√m54.6 ksi·√in

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 42 W/m·K24.3 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.2 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 300°C572 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

66 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
60%

Weldability

50 / 100
55 / 100

Formability (cold)

45 / 100
50 / 100

Same in both: Brazeability / Solderability 65 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 55 L/kg6.6 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM420

SCM420-CD vs SCM420-CR — frequently asked

Is SCM420-CD stronger than SCM420-CR?

Yes. SCM420-CD has a typical yield strength of 620 MPa (89.9 ksi) against 580 MPa (84.1 ksi) for SCM420-CR — about 7% more. Tensile strength is 760 MPa (110 ksi) vs 720 MPa (104 ksi).

Which condition does FabDigit quote by default, CD or CR?

HR is the default SCM420 condition in the FabDigit quote flow (neither CD nor CR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SCM420-CD or SCM420-CR?

SCM420-CD, by a small margin. Both rate good for machinability — 66/100 against 58/100 for SCM420-CR; for welding the order is SCM420-CR first (good, 55/100) then SCM420-CD (fair, 50/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in SCM420-CD and SCM420-CR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.