Steel S450J0 +AR vs S450J0 +N

Steel · S450J0 temper comparison

S450J0 +AR and S450J0 +N are two conditions of the same steel grade, S450J0: +AR (hot rolled) versus +N (normalized). The chemistry is identical, so every difference below comes from the condition. Both yield at about 480 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (hot rolled versus normalized). For most parts the choice follows the drawing's specified condition; ask for the one your standard calls out.

S450J0 +AR vs S450J0 +N: properties

S450J0 +ARS450J0 +N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

620 MPa89.9 ksi
610 MPa88.5 ksi

Yield Strength (0.2% offset)

480 MPa69.6 ksi
475 MPa68.9 ksi

Elongation at Break

20%
22%

Reduction in Area

45%
50%

Compressive Strength

480 MPa69.6 ksi
475 MPa68.9 ksi

Shear Strength

380 MPa55.1 ksi
375 MPa54.4 ksi

Fatigue Strength (Endurance Limit)

280 MPa40.6 ksi
285 MPa41.3 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
65 J47.9 ft·lbf

Hardness, Brinell

185 HB
180 HB

Hardness, Rockwell B

91 HRB
89 HRB

Hardness, Vickers

195 HV
190 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F

Max Service Temperature (continuous)

350°C662 °F
380°C716 °F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature 0°C32 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 9.5 % IACS · Electrical Resistivity 1.8×10⁻⁷ Ω·m7.09 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
47 / 100

Machinability Rating (AISI 1212 = 100 %)

52%
55%

Weldability

72 / 100
75 / 100

Formability (cold)

55 / 100
60 / 100

Same in both: Brazeability / Solderability 50 / 100 · Polishability 40 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleS450J0

S450J0 +AR vs S450J0 +N — frequently asked

What is the difference between S450J0 +AR and S450J0 +N?

S450J0 +AR and S450J0 +N are two conditions of the same steel grade, S450J0: +AR (hot rolled) versus +N (normalized). The chemistry is identical, so every difference below comes from the condition. Both yield at about 480 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (hot rolled versus normalized).

Which condition does FabDigit quote by default, +AR or +N?

+AR is the default S450J0 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S450J0 +AR and S450J0 +N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.