S420NL +N and S420NL +N 40-63 are two conditions of the same steel grade, S420NL: +N (normalized) versus +N 40-63 (+N). The chemistry is identical, so every difference below comes from the condition. S420NL +N is the stronger of the two: yield strength 450 MPa (65.3 ksi) against 420 MPa (60.9 ksi) for S420NL +N 40-63, about 7% more.

S420NL +NChoose it when strength drives the design.

S420NL +N vs S420NL +N 40-63: properties

S420NL +NS420NL +N 40-63

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

580 MPa84.1 ksi
560 MPa81.2 ksi

Yield Strength (0.2% offset)

450 MPa65.3 ksi
420 MPa60.9 ksi

Elongation at Break

24%
23%

Reduction in Area

55%
54%

Compressive Strength

450 MPa65.3 ksi
420 MPa60.9 ksi

Shear Strength

350 MPa50.8 ksi
336 MPa48.7 ksi

Fatigue Strength (Endurance Limit)

260 MPa37.7 ksi
250 MPa36.3 ksi

Fracture Toughness (K_IC)

120 MPa·√m109 ksi·√in
115 MPa·√m105 ksi·√in

Charpy V-Notch Impact (RT)

120 J88.5 ft·lbf
100 J73.8 ft·lbf

Hardness, Brinell

175 HB
168 HB

Hardness, Rockwell B

88 HRB
86 HRB

Hardness, Vickers

185 HV
177 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,500°C2,732 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 44 W/m·K25.4 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -50°C-58 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.2 % IACS · Electrical Resistivity 2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
56 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
61%

Weldability

85 / 100
84 / 100

Formability (cold)

65 / 100
62 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleS420NL

S420NL +N vs S420NL +N 40-63 — frequently asked

Is S420NL +N stronger than S420NL +N 40-63?

Yes. S420NL +N has a typical yield strength of 450 MPa (65.3 ksi) against 420 MPa (60.9 ksi) for S420NL +N 40-63 — about 7% more. Tensile strength is 580 MPa (84.1 ksi) vs 560 MPa (81.2 ksi).

Which condition does FabDigit quote by default, +N or +N 40-63?

+N is the default S420NL condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose S420NL +N over S420NL +N 40-63?

Pick S420NL +N when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S420NL +N and S420NL +N 40-63 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.