FabDigitFabDigit

Steel Q460-HR vs Q460-N

Steel · Q460 temper comparison

Q460-HR and Q460-N are two conditions of the same steel grade, Q460: HR (hot rolled) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. Both yield at about 500 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (hot rolled versus normalized). For most parts the choice follows the drawing's specified condition; ask for the one your standard calls out.

Q460-HR vs Q460-N: properties

Q460-HRQ460-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

620 MPa89.9 ksi
630 MPa91.4 ksi

Yield Strength (0.2% offset)

500 MPa72.5 ksi
505 MPa73.2 ksi

Elongation at Break

21%
22%

Reduction in Area

52%
56%

Compressive Strength

500 MPa72.5 ksi
505 MPa73.2 ksi

Shear Strength

375 MPa54.4 ksi
385 MPa55.8 ksi

Fatigue Strength (Endurance Limit)

265 MPa38.4 ksi
285 MPa41.3 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
115 MPa·√m105 ksi·√in

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
90 J66.4 ft·lbf

Same in both: Elastic (Young's) Modulus 206 GPa29.9 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Hardness, Brinell 185 HB · Hardness, Rockwell B 90 HRB · Hardness, Vickers 195 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

350°C662 °F
380°C716 °F

Min Service Temperature

0°C32 °F
-40°C-40 °F

Same in both: Thermal Conductivity 45 W/m·K26 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 260 J/g112 BTU/lb

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.2 % IACS · Electrical Resistivity 2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

52 / 100
54 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
57%

Weldability

70 / 100
74 / 100

Formability (cold)

55 / 100
60 / 100

Same in both: Castability 30 / 100 · Brazeability / Solderability 55 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleQ460

Q460-HR vs Q460-N — frequently asked

What is the difference between Q460-HR and Q460-N?

Q460-HR and Q460-N are two conditions of the same steel grade, Q460: HR (hot rolled) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. Both yield at about 500 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (hot rolled versus normalized).

Which condition does FabDigit quote by default, HR or N?

HR is the default Q460 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Q460-HR and Q460-N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.