Steel P460NH-N vs P460NH N-35-50

Steel · P460NH temper comparison

P460NH-N and P460NH N-35-50 are two conditions of the same steel grade, P460NH: N (normalized) versus N-35-50 (+N). The chemistry is identical, so every difference below comes from the condition. P460NH-N is the stronger of the two: yield strength 480 MPa (69.6 ksi) against 450 MPa (65.3 ksi) for P460NH N-35-50, about 7% more.

P460NH-NChoose it when strength drives the design.

P460NH-N vs P460NH N-35-50: properties

P460NH-NP460NH N-35-50

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

620 MPa89.9 ksi
610 MPa88.5 ksi

Yield Strength (0.2% offset)

480 MPa69.6 ksi
450 MPa65.3 ksi

Elongation at Break

22%
21%

Reduction in Area

55%
54%

Compressive Strength

480 MPa69.6 ksi
450 MPa65.3 ksi

Shear Strength

400 MPa58 ksi
380 MPa55.1 ksi

Fatigue Strength (Endurance Limit)

280 MPa40.6 ksi
270 MPa39.2 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
125 MPa·√m114 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
80 J59 ft·lbf

Hardness, Brinell

190 HB
182 HB

Hardness, Rockwell B

92 HRB
90 HRB

Hardness, Vickers

200 HV
191 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Hardness, Rockwell C 12 HRC

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 45 W/m·K26 BTU/hr·ft·°F · Specific Heat Capacity 461 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.2 % IACS · Electrical Resistivity 2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 14 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

52 / 100
54 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
57%

Weldability

78 / 100
77 / 100

Same in both: Formability (cold) 60 / 100 · Brazeability / Solderability 55 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 22%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP460NH

P460NH-N vs P460NH N-35-50 — frequently asked

Is P460NH-N stronger than P460NH N-35-50?

Yes. P460NH-N has a typical yield strength of 480 MPa (69.6 ksi) against 450 MPa (65.3 ksi) for P460NH N-35-50 — about 7% more. Tensile strength is 620 MPa (89.9 ksi) vs 610 MPa (88.5 ksi).

Which condition does FabDigit quote by default, N or N-35-50?

N is the default P460NH condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose P460NH-N over P460NH N-35-50?

Pick P460NH-N when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in P460NH-N and P460NH N-35-50 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.