Steel · P355NL2 temper comparison

P355NL2-N and P355NL2 N t50-100 are two conditions of the same steel grade, P355NL2: N (normalized) versus N t50-100 (n). The chemistry is identical, so every difference below comes from the condition. P355NL2-N is the stronger of the two: yield strength 385 MPa (55.8 ksi) against 350 MPa (50.8 ksi) for P355NL2 N t50-100, about 10% more.

P355NL2-NChoose it when strength drives the design.

P355NL2-N vs P355NL2 N t50-100: properties

P355NL2-NP355NL2 N t50-100

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

550 MPa79.8 ksi
525 MPa76.1 ksi

Yield Strength (0.2% offset)

385 MPa55.8 ksi
350 MPa50.8 ksi

Elongation at Break

26%
24%

Reduction in Area

55%
50%

Compressive Strength

385 MPa55.8 ksi
350 MPa50.8 ksi

Shear Strength

340 MPa49.3 ksi
315 MPa45.7 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
222 MPa32.2 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

180 J133 ft·lbf
140 J103 ft·lbf

Hardness, Brinell

155 HB
148 HB

Hardness, Rockwell B

82 HRB
79 HRB

Hardness, Vickers

163 HV
156 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 45 W/m·K26 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -50°C-58 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10.5 % IACS · Electrical Resistivity 1.65×10⁻⁷ Ω·m6.5 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
62 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
62%

Weldability

88 / 100
86 / 100

Formability (cold)

68 / 100
64 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 40 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP355NL2

P355NL2-N vs P355NL2 N t50-100 — frequently asked

Is P355NL2-N stronger than P355NL2 N t50-100?

Yes. P355NL2-N has a typical yield strength of 385 MPa (55.8 ksi) against 350 MPa (50.8 ksi) for P355NL2 N t50-100 — about 10% more. Tensile strength is 550 MPa (79.8 ksi) vs 525 MPa (76.1 ksi).

Which condition does FabDigit quote by default, N or N t50-100?

N is the default P355NL2 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose P355NL2-N over P355NL2 N t50-100?

Pick P355NL2-N when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in P355NL2-N and P355NL2 N t50-100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.