FabDigitFabDigit

Steel GX5NiS36-F vs GX5NiS36-SR

Steel · GX5NiS36 temper comparison

GX5NiS36-F and GX5NiS36-SR are two conditions of the same steel grade, GX5NiS36: F (as fabricated) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. GX5NiS36-F is the stronger of the two: yield strength 215 MPa (31.2 ksi) against 200 MPa (29 ksi) for GX5NiS36-SR, about 8% more. In exchange, GX5NiS36-SR is the more ductile: elongation 12% versus 10% for GX5NiS36-F, and GX5NiS36-F is harder (145 HB vs 135 HB).

GX5NiS36-FChoose it when strength drives the design.

GX5NiS36-SRChoose it when the part is bent, formed or impact-loaded.

GX5NiS36-F vs GX5NiS36-SR: properties

GX5NiS36-FGX5NiS36-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

138 GPa20 Msi
140 GPa20.3 Msi

Tensile Strength (Ultimate)

430 MPa62.4 ksi
420 MPa60.9 ksi

Yield Strength (0.2% offset)

215 MPa31.2 ksi
200 MPa29 ksi

Elongation at Break

10%
12%

Reduction in Area

15%
20%

Compressive Strength

440 MPa63.8 ksi
430 MPa62.4 ksi

Shear Strength

310 MPa45 ksi
300 MPa43.5 ksi

Fatigue Strength (Endurance Limit)

150 MPa21.8 ksi
160 MPa23.2 ksi

Fracture Toughness (K_IC)

50 MPa·√m45.5 ksi·√in
58 MPa·√m52.8 ksi·√in

Charpy V-Notch Impact (RT)

16 J11.8 ft·lbf
20 J14.8 ft·lbf

Hardness, Brinell

145 HB
135 HB

Hardness, Rockwell B

78 HRB
75 HRB

Hardness, Vickers

152 HV
142 HV

Same in both: Shear Modulus 55 GPa8 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 8.1 g/cm³0.29 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

11.2 W/m·K6.5 BTU/hr·ft·°F
11.5 W/m·K6.6 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

3.4 µm/m·K1.9 µin/in·°F
3 µm/m·K1.7 µin/in·°F

Same in both: Specific Heat Capacity 515 J/kg·K0.12 BTU/lb·°F · Latent Heat of Fusion 275 J/g118 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -150°C-238 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.1 % IACS
2.1 % IACS

Electrical Resistivity

8.4×10⁻⁷ Ω·m33.1 µΩ·in
8.2×10⁻⁷ Ω·m32.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

28 / 100
30 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

38 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

33%
35%

Weldability

22 / 100
25 / 100

Formability (cold)

8 / 100
10 / 100

Same in both: Castability 60 / 100 · Brazeability / Solderability 55 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 110 MJ/kg47,292 BTU/lb · Embodied Carbon (primary production) 8.5 kg CO₂/kg · Embodied Water 300 L/kg35.9 gal/lb · Typical Recycled Content 35%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGX5NiS36

GX5NiS36-F vs GX5NiS36-SR — frequently asked

Is GX5NiS36-F stronger than GX5NiS36-SR?

Yes. GX5NiS36-F has a typical yield strength of 215 MPa (31.2 ksi) against 200 MPa (29 ksi) for GX5NiS36-SR — about 8% more. Tensile strength is 430 MPa (62.4 ksi) vs 420 MPa (60.9 ksi).

Which condition does FabDigit quote by default, F or SR?

SR is the default GX5NiS36 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose GX5NiS36-F over GX5NiS36-SR?

Pick GX5NiS36-F when strength drives the design. Pick GX5NiS36-SR when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in GX5NiS36-F and GX5NiS36-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.