FabDigitFabDigit

Steel GX3Ni36-A vs GX3Ni36-SR

Steel · GX3Ni36 temper comparison

GX3Ni36-A and GX3Ni36-SR are two conditions of the same steel grade, GX3Ni36: A (solution annealed) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. GX3Ni36-SR is the stronger of the two: yield strength 235 MPa (34.1 ksi) against 205 MPa (29.7 ksi) for GX3Ni36-A, about 15% more. In exchange, GX3Ni36-A is the more ductile: elongation 30% versus 27% for GX3Ni36-SR, and GX3Ni36-SR is harder (128 HB vs 120 HB).

GX3Ni36-AChoose it when the part is bent, formed or impact-loaded.

GX3Ni36-SRChoose it when strength drives the design.

GX3Ni36-A vs GX3Ni36-SR: properties

GX3Ni36-AGX3Ni36-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

144 GPa20.9 Msi
142 GPa20.6 Msi

Tensile Strength (Ultimate)

425 MPa61.6 ksi
445 MPa64.5 ksi

Yield Strength (0.2% offset)

205 MPa29.7 ksi
235 MPa34.1 ksi

Elongation at Break

30%
27%

Reduction in Area

42%
36%

Compressive Strength

210 MPa30.5 ksi
240 MPa34.8 ksi

Shear Strength

300 MPa43.5 ksi
315 MPa45.7 ksi

Fatigue Strength (Endurance Limit)

190 MPa27.6 ksi
205 MPa29.7 ksi

Fracture Toughness (K_IC)

95 MPa·√m86.5 ksi·√in
85 MPa·√m77.4 ksi·√in

Charpy V-Notch Impact (RT)

75 J55.3 ft·lbf
65 J47.9 ft·lbf

Hardness, Brinell

120 HB
128 HB

Hardness, Rockwell B

67 HRB
71 HRB

Hardness, Vickers

126 HV
135 HV

Same in both: Shear Modulus 55 GPa8 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 8.1 g/cm³0.29 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

10.7 W/m·K6.2 BTU/hr·ft·°F
11 W/m·K6.4 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

1.6 µm/m·K0.89 µin/in·°F
2 µm/m·K1.1 µin/in·°F

Same in both: Specific Heat Capacity 515 J/kg·K0.12 BTU/lb·°F · Latent Heat of Fusion 275 J/g118 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.2 % IACS
2.1 % IACS

Electrical Resistivity

7.9×10⁻⁷ Ω·m31.1 µΩ·in
8.1×10⁻⁷ Ω·m31.9 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.35 V · Corrosion Resistance 25 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
31 / 100

Machinability Rating (AISI 1212 = 100 %)

27%
26%

Weldability

65 / 100
62 / 100

Formability (cold)

30 / 100
24 / 100

Same in both: Castability 50 / 100 · Brazeability / Solderability 65 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 90 MJ/kg38,693 BTU/lb · Embodied Carbon (primary production) 7 kg CO₂/kg · Embodied Water 200 L/kg24 gal/lb · Typical Recycled Content 45%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGX3Ni36

GX3Ni36-A vs GX3Ni36-SR — frequently asked

Is GX3Ni36-SR stronger than GX3Ni36-A?

Yes. GX3Ni36-SR has a typical yield strength of 235 MPa (34.1 ksi) against 205 MPa (29.7 ksi) for GX3Ni36-A — about 15% more. Tensile strength is 445 MPa (64.5 ksi) vs 425 MPa (61.6 ksi).

Which condition does FabDigit quote by default, A or SR?

F is the default GX3Ni36 condition in the FabDigit quote flow (neither A nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose GX3Ni36-A over GX3Ni36-SR?

Pick GX3Ni36-A when the part is bent, formed or impact-loaded. Pick GX3Ni36-SR when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in GX3Ni36-A and GX3Ni36-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.