FabDigitFabDigit

Steel GE270 +NT vs GE270 +SR

Steel · GE270 temper comparison

GE270 +NT and GE270 +SR are two conditions of the same steel grade, GE270: +NT (normalized and tempered) versus +SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. GE270 +NT is the stronger of the two: yield strength 305 MPa (44.2 ksi) against 275 MPa (39.9 ksi) for GE270 +SR, about 11% more; tensile strength follows at 525 MPa (76.1 ksi) vs 495 MPa (71.8 ksi). GE270 +NT is the more ductile: elongation 22% versus 18% for GE270 +SR, and GE270 +NT is harder (158 HB vs 148 HB).

GE270 +NTChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

GE270 +NT vs GE270 +SR: properties

GE270 +NTGE270 +SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

525 MPa76.1 ksi
495 MPa71.8 ksi

Yield Strength (0.2% offset)

305 MPa44.2 ksi
275 MPa39.9 ksi

Elongation at Break

22%
18%

Reduction in Area

40%
30%

Compressive Strength

305 MPa44.2 ksi
275 MPa39.9 ksi

Shear Strength

325 MPa47.1 ksi
305 MPa44.2 ksi

Fatigue Strength (Endurance Limit)

235 MPa34.1 ksi
205 MPa29.7 ksi

Fracture Toughness (K_IC)

78 MPa·√m71 ksi·√in
62 MPa·√m56.4 ksi·√in

Charpy V-Notch Impact (RT)

38 J28 ft·lbf
24 J17.7 ft·lbf

Hardness, Brinell

158 HB
148 HB

Hardness, Rockwell B

83 HRB
79 HRB

Hardness, Vickers

166 HV
156 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,505°C2,741 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

425°C797 °F
400°C752 °F

Same in both: Thermal Conductivity 48 W/m·K27.7 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

61 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

64%
62%

Weldability

78 / 100
80 / 100

Formability (cold)

16 / 100
14 / 100

Same in both: Castability 78 / 100 · Brazeability / Solderability 55 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 24 MJ/kg10,318 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 55 L/kg6.6 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE270

GE270 +NT vs GE270 +SR — frequently asked

Is GE270 +NT stronger than GE270 +SR?

Yes. GE270 +NT has a typical yield strength of 305 MPa (44.2 ksi) against 275 MPa (39.9 ksi) for GE270 +SR — about 11% more. Tensile strength is 525 MPa (76.1 ksi) vs 495 MPa (71.8 ksi).

Which condition does FabDigit quote by default, +NT or +SR?

+N is the default GE270 condition in the FabDigit quote flow (neither +NT nor +SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose GE270 +NT over GE270 +SR?

Pick GE270 +NT when strength drives the design, or when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in GE270 +NT and GE270 +SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.