G9Ni14-NT and G9Ni14-QT are two conditions of the same steel grade, G9Ni14: NT (double) normalized and tempered) versus QT (quenched and tempered). The chemistry is identical, so every difference below comes from the condition. Both yield at about 385 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (double) normalized and tempered versus quenched and tempered). For most parts the choice follows the drawing's specified condition; ask for the one your standard calls out.

G9Ni14-NT vs G9Ni14-QT: properties

G9Ni14-NTG9Ni14-QT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
204 GPa29.6 Msi

Tensile Strength (Ultimate)

540 MPa78.3 ksi
560 MPa81.2 ksi

Yield Strength (0.2% offset)

385 MPa55.8 ksi
400 MPa58 ksi

Elongation at Break

26%
25%

Compressive Strength

385 MPa55.8 ksi
400 MPa58 ksi

Shear Strength

325 MPa47.1 ksi
340 MPa49.3 ksi

Fatigue Strength (Endurance Limit)

225 MPa32.6 ksi
235 MPa34.1 ksi

Fracture Toughness (K_IC)

120 MPa·√m109 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

100 J73.8 ft·lbf
110 J81.1 ft·lbf

Hardness, Brinell

168 HB
175 HB

Hardness, Rockwell B

86 HRB
88 HRB

Hardness, Vickers

177 HV
185 HV

Same in both: Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.29 · Reduction in Area 55%

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,440°C2,624 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

34 W/m·K19.6 BTU/hr·ft·°F
32 W/m·K18.5 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.5 µm/m·K6.4 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 300°C572 °F · Min Service Temperature -100°C-148 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

6.2 % IACS
5.8 % IACS

Electrical Resistivity

2.8×10⁻⁷ Ω·m11 µΩ·in
3×10⁻⁷ Ω·m11.8 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 15 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
58%

Formability (cold)

27 / 100
25 / 100

Same in both: Weldability 65 / 100 · Castability 65 / 100 · Brazeability / Solderability 45 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 31 MJ/kg13,328 BTU/lb · Embodied Carbon (primary production) 2.4 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 75%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleG9Ni14

G9Ni14-NT vs G9Ni14-QT — frequently asked

What is the difference between G9Ni14-NT and G9Ni14-QT?

G9Ni14-NT and G9Ni14-QT are two conditions of the same steel grade, G9Ni14: NT (double) normalized and tempered) versus QT (quenched and tempered). The chemistry is identical, so every difference below comes from the condition. Both yield at about 385 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (double) normalized and tempered versus quenched and tempered).

Which condition does FabDigit quote by default, NT or QT?

QT is the default G9Ni14 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Ready to make it?

Upload a CAD file and FabDigit prices the part in G9Ni14-NT and G9Ni14-QT side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.