FabDigitFabDigit

Steel E7018-AW vs E7018-SR

Steel · E7018 temper comparison

E7018-AW and E7018-SR are two conditions of the same steel grade, E7018: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. E7018-AW is the stronger of the two: yield strength 450 MPa (65.3 ksi) against 420 MPa (60.9 ksi) for E7018-SR, about 7% more. E7018-AW is harder — 170 HB against 155 HB for E7018-SR — which matters for wear surfaces and threads.

E7018-AWChoose it when strength drives the design, or when surface hardness matters.

E7018-AW vs E7018-SR: properties

E7018-AWE7018-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

540 MPa78.3 ksi
515 MPa74.7 ksi

Yield Strength (0.2% offset)

450 MPa65.3 ksi
420 MPa60.9 ksi

Elongation at Break

28%
30%

Reduction in Area

65%
70%

Charpy V-Notch Impact (RT)

130 J95.9 ft·lbf
140 J103 ft·lbf

Hardness, Brinell

170 HB
155 HB

Hardness, Vickers

180 HV
163 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Shear Strength 330 MPa47.9 ksi · Fatigue Strength (Endurance Limit) 220 MPa31.9 ksi · Fracture Toughness (K_IC) 120 MPa·√m109 ksi·√in · Hardness, Rockwell B 87 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,465°C2,669 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

400°C752 °F
425°C797 °F

Same in both: Thermal Conductivity 50 W/m·K28.9 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 11 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability Rating (AISI 1212 = 100 %)

60%
68%

Same in both: Machinability 55 / 100 · Weldability 95 / 100 · Formability (cold) 55 / 100 · Brazeability / Solderability 70 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 33 MJ/kg14,187 BTU/lb · Embodied Carbon (primary production) 2.6 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleE7018

E7018-AW vs E7018-SR — frequently asked

Is E7018-AW stronger than E7018-SR?

Yes. E7018-AW has a typical yield strength of 450 MPa (65.3 ksi) against 420 MPa (60.9 ksi) for E7018-SR — about 7% more. Tensile strength is 540 MPa (78.3 ksi) vs 515 MPa (74.7 ksi).

Which condition does FabDigit quote by default, AW or SR?

AW is the default E7018 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose E7018-AW over E7018-SR?

Pick E7018-AW when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in E7018-AW and E7018-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.