FabDigitFabDigit

Steel A516 Gr 70 Annealed vs A516 Gr 70 Normalized

Steel · A516 Gr 70 temper comparison

A516 Gr 70 Annealed and A516 Gr 70 Normalized are two conditions of the same steel grade, A516 Gr 70: Annealed versus Normalized. The chemistry is identical, so every difference below comes from the condition. A516 Gr 70 Normalized is the stronger of the two: yield strength 315 MPa (45.7 ksi) against 290 MPa (42.1 ksi) for A516 Gr 70 Annealed, about 9% more; tensile strength follows at 540 MPa (78.3 ksi) vs 505 MPa (73.2 ksi).

A516 Gr 70 NormalizedChoose it when strength drives the design.

A516 Gr 70 Annealed vs A516 Gr 70 Normalized: properties

A516 Gr 70 AnnealedA516 Gr 70 Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

505 MPa73.2 ksi
540 MPa78.3 ksi

Yield Strength (0.2% offset)

290 MPa42.1 ksi
315 MPa45.7 ksi

Elongation at Break

28%
27%

Fatigue Strength (Endurance Limit)

225 MPa32.6 ksi
245 MPa35.5 ksi

Fracture Toughness (K_IC)

110 MPa·√m100 ksi·√in
150 MPa·√m137 ksi·√in

Charpy V-Notch Impact (RT)

50 J36.9 ft·lbf
95 J70.1 ft·lbf

Hardness, Brinell

140 HB
146 HB

Hardness, Rockwell B

76 HRB
78 HRB

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Reduction in Area 55% · Compressive Strength 320 MPa46.4 ksi · Shear Strength 350 MPa50.8 ksi · Hardness, Vickers 158 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Min Service Temperature

-29°C-20 °F
-46°C-51 °F

Same in both: Thermal Conductivity 52 W/m·K30 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb · Max Service Temperature (continuous) 425°C797 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

66 / 100
60 / 100

Machinability Rating (AISI 1212 = 100 %)

72%
66%

Formability (cold)

82 / 100
74 / 100

Same in both: Weldability 90 / 100 · Brazeability / Solderability 70 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA516 Gr 70

A516 Gr 70 Annealed vs A516 Gr 70 Normalized — frequently asked

Is A516 Gr 70 Normalized stronger than A516 Gr 70 Annealed?

Yes. A516 Gr 70 Normalized has a typical yield strength of 315 MPa (45.7 ksi) against 290 MPa (42.1 ksi) for A516 Gr 70 Annealed — about 9% more. Tensile strength is 540 MPa (78.3 ksi) vs 505 MPa (73.2 ksi).

Which condition does FabDigit quote by default, Annealed or Normalized?

HR is the default A516 Gr 70 condition in the FabDigit quote flow (neither Annealed nor Normalized). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, A516 Gr 70 Annealed or A516 Gr 70 Normalized?

A516 Gr 70 Annealed, by a small margin. Both rate good for machinability — 66/100 against 60/100 for A516 Gr 70 Normalized.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A516 Gr 70 Annealed and A516 Gr 70 Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.