FabDigitFabDigit

Steel A514 Gr B vs A514-T5

Steel · A514 temper comparison

A514 Gr B and A514-T5 are two conditions of the same steel grade, A514: Gr B (grade B) versus T5 (cooled from hot working and artificially aged). The chemistry is identical, so every difference below comes from the condition. A514 Gr B is the stronger of the two: yield strength 740 MPa (107 ksi) against 690 MPa (100 ksi) for A514-T5, about 7% more; tensile strength follows at 810 MPa (117 ksi) vs 760 MPa (110 ksi). A514 Gr B is harder — 258 HB against 235 HB for A514-T5 — which matters for wear surfaces and threads.

A514 Gr BChoose it when strength drives the design, or when surface hardness matters.

A514 Gr B vs A514-T5: properties

A514 Gr BA514-T5

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

810 MPa117 ksi
760 MPa110 ksi

Yield Strength (0.2% offset)

740 MPa107 ksi
690 MPa100 ksi

Elongation at Break

19%
20%

Reduction in Area

50%
52%

Compressive Strength

760 MPa110 ksi
690 MPa100 ksi

Shear Strength

495 MPa71.8 ksi
460 MPa66.7 ksi

Fatigue Strength (Endurance Limit)

375 MPa54.4 ksi
350 MPa50.8 ksi

Fracture Toughness (K_IC)

115 MPa·√m105 ksi·√in
100 MPa·√m91 ksi·√in

Hardness, Brinell

258 HB
235 HB

Hardness, Rockwell C

26 HRC
21 HRC

Hardness, Vickers

272 HV
247 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Charpy V-Notch Impact (RT) 60 J44.3 ft·lbf · Hardness, Rockwell B 100 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

41 W/m·K23.7 BTU/hr·ft·°F
43 W/m·K24.8 BTU/hr·ft·°F

Specific Heat Capacity

480 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12.2 µm/m·K6.8 µin/in·°F
12 µm/m·K6.7 µin/in·°F

Min Service Temperature

-40°C-40 °F
-45°C-49 °F

Same in both: Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7 % IACS · Electrical Resistivity 2.4×10⁻⁷ Ω·m9.45 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

14 / 100
16 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

37 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

32%
42%

Weldability

58 / 100
57 / 100

Formability (cold)

35 / 100
33 / 100

Same in both: Brazeability / Solderability 40 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.4 kg CO₂/kg

Same in both: Embodied Energy (primary production) 31 MJ/kg13,328 BTU/lb · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA514

A514 Gr B vs A514-T5 — frequently asked

Is A514 Gr B stronger than A514-T5?

Yes. A514 Gr B has a typical yield strength of 740 MPa (107 ksi) against 690 MPa (100 ksi) for A514-T5 — about 7% more. Tensile strength is 810 MPa (117 ksi) vs 760 MPa (110 ksi).

Which condition does FabDigit quote by default, Gr B or T5?

Q&T is the default A514 condition in the FabDigit quote flow (neither Gr B nor T5). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose A514 Gr B over A514-T5?

Pick A514 Gr B when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A514 Gr B and A514-T5 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.