FabDigitFabDigit

Steel 5130-CD vs 5130-HR

Steel · 5130 temper comparison

5130-CD and 5130-HR are two conditions of the same steel grade, 5130: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. 5130-CD is the stronger of the two: yield strength 580 MPa (84.1 ksi) against 415 MPa (60.2 ksi) for 5130-HR, about 40% more; tensile strength follows at 680 MPa (98.6 ksi) vs 635 MPa (92.1 ksi). In exchange, 5130-HR is the more ductile: elongation 22% versus 12% for 5130-CD, and 5130-CD is harder (200 HB vs 187 HB).

5130-CDChoose it when strength drives the design.

5130-HRChoose it when the part is bent, formed or impact-loaded.

5130-CD vs 5130-HR: properties

5130-CD5130-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

680 MPa98.6 ksi
635 MPa92.1 ksi

Yield Strength (0.2% offset)

580 MPa84.1 ksi
415 MPa60.2 ksi

Elongation at Break

12%
22%

Reduction in Area

42%
55%

Shear Strength

410 MPa59.5 ksi
420 MPa60.9 ksi

Charpy V-Notch Impact (RT)

30 J22.1 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

200 HB
187 HB

Hardness, Rockwell B

93 HRB
90 HRB

Hardness, Vickers

210 HV
196 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Compressive Strength 415 MPa60.2 ksi · Fatigue Strength (Endurance Limit) 300 MPa43.5 ksi · Fracture Toughness (K_IC) 100 MPa·√m91 ksi·√in

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Specific Heat Capacity

475 J/kg·K0.11 BTU/lb·°F
477 J/kg·K0.11 BTU/lb·°F

Same in both: Thermal Expansion (CTE, 20–100 °C) 12.2 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
65%

Weldability

40 / 100
45 / 100

Formability (cold)

35 / 100
50 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

34 MJ/kg14,617 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
1.9 kg CO₂/kg

Same in both: Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale5130

5130-CD vs 5130-HR — frequently asked

Is 5130-CD stronger than 5130-HR?

Yes. 5130-CD has a typical yield strength of 580 MPa (84.1 ksi) against 415 MPa (60.2 ksi) for 5130-HR — about 40% more. Tensile strength is 680 MPa (98.6 ksi) vs 635 MPa (92.1 ksi).

Which condition does FabDigit quote by default, CD or HR?

HR is the default 5130 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 5130-CD or 5130-HR?

5130-HR. Its weldability rates fair (45/100) against fair (40/100) for 5130-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 5130-CD and 5130-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.