Steel 4620-CD vs 4620-HR

Steel · 4620 temper comparison

4620-CD and 4620-HR are two conditions of the same steel grade, 4620: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. 4620-CD is the stronger of the two: yield strength 550 MPa (79.8 ksi) against 360 MPa (52.2 ksi) for 4620-HR, about 53% more; tensile strength follows at 640 MPa (92.8 ksi) vs 570 MPa (82.7 ksi). In exchange, 4620-HR is the more ductile: elongation 26% versus 17% for 4620-CD, and 4620-CD is harder (192 HB vs 163 HB).

4620-CDChoose it when strength drives the design.

4620-HRChoose it when the part is bent, formed or impact-loaded.

4620-CD vs 4620-HR: properties

4620-CD4620-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

640 MPa92.8 ksi
570 MPa82.7 ksi

Yield Strength (0.2% offset)

550 MPa79.8 ksi
360 MPa52.2 ksi

Elongation at Break

17%
26%

Reduction in Area

50%
55%

Shear Strength

385 MPa55.8 ksi
380 MPa55.1 ksi

Fatigue Strength (Endurance Limit)

290 MPa42.1 ksi
260 MPa37.7 ksi

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
85 J62.7 ft·lbf

Hardness, Brinell

192 HB
163 HB

Hardness, Rockwell B

92 HRB
84 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,425°C2,597 °F
1,420°C2,588 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Expansion (CTE, 20–100 °C)

12.2 µm/m·K6.8 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Min Service Temperature

-40°C-40 °F
-50°C-58 °F

Same in both: Thermal Conductivity 46 W/m·K26.6 BTU/hr·ft·°F · Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
57 / 100

Weldability

60 / 100
65 / 100

Formability (cold)

45 / 100
58 / 100

Polishability

60 / 100
55 / 100

Same in both: Machinability Rating (AISI 1212 = 100 %) 65% · Brazeability / Solderability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

34 MJ/kg14,617 BTU/lb
29 MJ/kg12,468 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.2 kg CO₂/kg

Typical Recycled Content

35%
30%

Same in both: Embodied Water 55 L/kg6.6 gal/lb

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4620

4620-CD vs 4620-HR — frequently asked

Is 4620-CD stronger than 4620-HR?

Yes. 4620-CD has a typical yield strength of 550 MPa (79.8 ksi) against 360 MPa (52.2 ksi) for 4620-HR — about 53% more. Tensile strength is 640 MPa (92.8 ksi) vs 570 MPa (82.7 ksi).

Which condition does FabDigit quote by default, CD or HR?

HR is the default 4620 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 4620-CD or 4620-HR?

4620-HR. Its weldability rates good (65/100) against good (60/100) for 4620-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4620-CD and 4620-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.