4620 Annealed and 4620-CD are two conditions of the same steel grade, 4620: Annealed versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. 4620-CD is the stronger of the two: yield strength 550 MPa (79.8 ksi) against 372 MPa (54 ksi) for 4620 Annealed, about 48% more; tensile strength follows at 640 MPa (92.8 ksi) vs 512 MPa (74.3 ksi). In exchange, 4620 Annealed is the more ductile: elongation 31.3% versus 17% for 4620-CD, and 4620-CD is harder (192 HB vs 149 HB).

4620 AnnealedChoose it when the part is bent, formed or impact-loaded.

4620-CDChoose it when strength drives the design.

4620 Annealed vs 4620-CD: properties

4620 Annealed4620-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

512 MPa74.3 ksi
640 MPa92.8 ksi

Yield Strength (0.2% offset)

372 MPa54 ksi
550 MPa79.8 ksi

Elongation at Break

31.3%
17%

Reduction in Area

60%
50%

Shear Strength

380 MPa55.1 ksi
385 MPa55.8 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
290 MPa42.1 ksi

Charpy V-Notch Impact (RT)

95 J70.1 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

149 HB
192 HB

Hardness, Rockwell B

80 HRB
92 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,420°C2,588 °F
1,425°C2,597 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Expansion (CTE, 20–100 °C)

11.9 µm/m·K6.6 µin/in·°F
12.2 µm/m·K6.8 µin/in·°F

Min Service Temperature

-50°C-58 °F
-40°C-40 °F

Same in both: Thermal Conductivity 46 W/m·K26.6 BTU/hr·ft·°F · Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability Rating (AISI 1212 = 100 %)

66%
65%

Weldability

65 / 100
60 / 100

Formability (cold)

70 / 100
45 / 100

Polishability

55 / 100
60 / 100

Same in both: Machinability 60 / 100 · Brazeability / Solderability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

29 MJ/kg12,468 BTU/lb
34 MJ/kg14,617 BTU/lb

Embodied Carbon (primary production)

2.2 kg CO₂/kg
2.3 kg CO₂/kg

Typical Recycled Content

30%
35%

Same in both: Embodied Water 55 L/kg6.6 gal/lb

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4620

4620 Annealed vs 4620-CD — frequently asked

Is 4620-CD stronger than 4620 Annealed?

Yes. 4620-CD has a typical yield strength of 550 MPa (79.8 ksi) against 372 MPa (54 ksi) for 4620 Annealed — about 48% more. Tensile strength is 640 MPa (92.8 ksi) vs 512 MPa (74.3 ksi).

Which condition does FabDigit quote by default, Annealed or CD?

HR is the default 4620 condition in the FabDigit quote flow (neither Annealed nor CD). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 4620 Annealed or 4620-CD?

4620 Annealed. Its weldability rates good (65/100) against good (60/100) for 4620-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4620 Annealed and 4620-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.