Steel 45B-CD vs 45B-HR

Steel · 45B temper comparison

45B-CD and 45B-HR are two conditions of the same steel grade, 45B: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. 45B-CD is the stronger of the two: yield strength 620 MPa (89.9 ksi) against 400 MPa (58 ksi) for 45B-HR, about 55% more; tensile strength follows at 780 MPa (113 ksi) vs 700 MPa (102 ksi). In exchange, 45B-HR is the more ductile: elongation 16% versus 10% for 45B-CD, and 45B-CD is harder (235 HB vs 197 HB). 45B-HR runs hotter in service (400°C vs 300°C continuous).

45B-CDChoose it when strength drives the design.

45B-HRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

45B-CD vs 45B-HR: properties

45B-CD45B-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

780 MPa113 ksi
700 MPa102 ksi

Yield Strength (0.2% offset)

620 MPa89.9 ksi
400 MPa58 ksi

Elongation at Break

10%
16%

Reduction in Area

35%
40%

Compressive Strength

620 MPa89.9 ksi
400 MPa58 ksi

Shear Strength

470 MPa68.2 ksi
450 MPa65.3 ksi

Fatigue Strength (Endurance Limit)

340 MPa49.3 ksi
320 MPa46.4 ksi

Charpy V-Notch Impact (RT)

18 J13.3 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

235 HB
197 HB

Hardness, Rockwell B

99 HRB
92 HRB

Hardness, Vickers

247 HV
207 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
400°C752 °F

Same in both: Thermal Conductivity 46 W/m·K26.6 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.6 µm/m·K6.4 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8.5 % IACS
8.6 % IACS

Electrical Resistivity

2.03×10⁻⁷ Ω·m7.99 µΩ·in
2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
58%

Weldability

35 / 100
40 / 100

Formability (cold)

25 / 100
40 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale45B

45B-CD vs 45B-HR — frequently asked

Is 45B-CD stronger than 45B-HR?

Yes. 45B-CD has a typical yield strength of 620 MPa (89.9 ksi) against 400 MPa (58 ksi) for 45B-HR — about 55% more. Tensile strength is 780 MPa (113 ksi) vs 700 MPa (102 ksi).

Which condition does FabDigit quote by default, CD or HR?

HR is the default 45B condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 45B-CD or 45B-HR?

45B-CD, by a small margin. Both rate good for machinability — 62/100 against 55/100 for 45B-HR; for welding the order is 45B-HR first (fair, 40/100) then 45B-CD (fair, 35/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in 45B-CD and 45B-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.