FabDigitFabDigit

Steel 4023-A vs 4023-CD

Steel · 4023 temper comparison

4023-A and 4023-CD are two conditions of the same steel grade, 4023: A (solution annealed) versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. 4023-CD is the stronger of the two: yield strength 470 MPa (68.2 ksi) against 290 MPa (42.1 ksi) for 4023-A, about 62% more; tensile strength follows at 552 MPa (80.1 ksi) vs 448 MPa (65 ksi). In exchange, 4023-A is the more ductile: elongation 28% versus 18% for 4023-CD, and 4023-CD is harder (163 HB vs 137 HB).

4023-AChoose it when the part is bent, formed or impact-loaded.

4023-CDChoose it when strength drives the design.

4023-A vs 4023-CD: properties

4023-A4023-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

448 MPa65 ksi
552 MPa80.1 ksi

Yield Strength (0.2% offset)

290 MPa42.1 ksi
470 MPa68.2 ksi

Elongation at Break

28%
18%

Reduction in Area

60%
50%

Fatigue Strength (Endurance Limit)

210 MPa30.5 ksi
250 MPa36.3 ksi

Charpy V-Notch Impact (RT)

75 J55.3 ft·lbf
55 J40.6 ft·lbf

Hardness, Brinell

137 HB
163 HB

Hardness, Rockwell B

75 HRB
84 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Shear Strength 360 MPa52.2 ksi · Fracture Toughness (K_IC) 95 MPa·√m86.5 ksi·√in · Hardness, Vickers 171 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 43 W/m·K24.8 BTU/hr·ft·°F · Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.2 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
65 / 100

Weldability

80 / 100
74 / 100

Formability (cold)

72 / 100
50 / 100

Same in both: Machinability Rating (AISI 1212 = 100 %) 70% · Brazeability / Solderability 60 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4023

4023-A vs 4023-CD — frequently asked

Is 4023-CD stronger than 4023-A?

Yes. 4023-CD has a typical yield strength of 470 MPa (68.2 ksi) against 290 MPa (42.1 ksi) for 4023-A — about 62% more. Tensile strength is 552 MPa (80.1 ksi) vs 448 MPa (65 ksi).

Which condition does FabDigit quote by default, A or CD?

CD is the default 4023 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 4023-A or 4023-CD?

4023-A. Its weldability rates very good (80/100) against very good (74/100) for 4023-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4023-A and 4023-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.