Steel 1211-CD vs 1211 CD-SR
Steel · 1211 temper comparison
1211-CD and 1211 CD-SR are two conditions of the same steel grade, 1211: CD (cold drawn) versus CD-SR (cold drawn, stress relieved). The chemistry is identical, so every difference below comes from the condition. 1211-CD is the stronger of the two: yield strength 470 MPa (68.2 ksi) against 430 MPa (62.4 ksi) for 1211 CD-SR, about 9% more. In exchange, 1211 CD-SR is the more ductile: elongation 13% versus 10% for 1211-CD.
1211-CDChoose it when strength drives the design.
1211 CD-SRChoose it when the part is bent, formed or impact-loaded.
1211-CD vs 1211 CD-SR: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Tensile Strength (Ultimate)
Yield Strength (0.2% offset)
Elongation at Break
Reduction in Area
Compressive Strength
Shear Strength
Fatigue Strength (Endurance Limit)
Charpy V-Notch Impact (RT)
Hardness, Brinell
Hardness, Rockwell B
Hardness, Vickers
Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 140 GPa20.3 Msi · Poisson's Ratio 0.29
Physical
Density and transition temperatures.
Same in both: Density 7.87 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,505°C2,741 °F
Thermal
How each material carries heat and how hot it can run.
Same in both: Thermal Conductivity 51 W/m·K29.5 BTU/hr·ft·°F · Specific Heat Capacity 480 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.9 µm/m·K6.6 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -20°C-4 °F
Electrical
Conductivity and insulation.
Same in both: Electrical Conductivity 10.8 % IACS · Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 8 / 100
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Formability (cold)
Same in both: Machinability 90 / 100 · Machinability Rating (AISI 1212 = 100 %) 95% · Weldability 20 / 100 · Brazeability / Solderability 55 / 100 · Polishability 45 / 100
Sustainability
Primary-production footprint per kilogram.
Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%
Strength versus weight
Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
1211-CD vs 1211 CD-SR — frequently asked
Is 1211-CD stronger than 1211 CD-SR?
Yes. 1211-CD has a typical yield strength of 470 MPa (68.2 ksi) against 430 MPa (62.4 ksi) for 1211 CD-SR — about 9% more. Tensile strength is 540 MPa (78.3 ksi) vs 515 MPa (74.7 ksi).
Which condition does FabDigit quote by default, CD or CD-SR?
CD is the default 1211 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.
When should I choose 1211-CD over 1211 CD-SR?
Pick 1211-CD when strength drives the design. Pick 1211 CD-SR when the part is bent, formed or impact-loaded.
Ready to make it?
Upload a CAD file and FabDigit prices the part in 1211-CD and 1211 CD-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.