Stainless Steel S44627 Annealed vs S44627 As Welded

Stainless Steel · S44627 temper comparison

S44627 Annealed and S44627 As Welded are two conditions of the same stainless steel grade, S44627: Annealed versus As Welded (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 345 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (Annealed versus as-welded deposit). S44627 Annealed is the more ductile: elongation 30% versus 12% for S44627 As Welded, and S44627 As Welded is harder (175 HB vs 160 HB).

S44627 AnnealedChoose it when the part is bent, formed or impact-loaded.

S44627 Annealed vs S44627 As Welded: properties

S44627 AnnealedS44627 As Welded

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Yield Strength (0.2% offset)

345 MPa50 ksi
350 MPa50.8 ksi

Elongation at Break

30%
12%

Reduction in Area

60%
25%

Compressive Strength

345 MPa50 ksi
350 MPa50.8 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
170 MPa24.7 ksi

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
8 J5.9 ft·lbf

Hardness, Brinell

160 HB
175 HB

Hardness, Rockwell B

84 HRB
87 HRB

Hardness, Vickers

170 HV
185 HV

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Tensile Strength (Ultimate) 490 MPa71.1 ksi · Shear Strength 300 MPa43.5 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.67 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Min Service Temperature

-30°C-22 °F
20°C68 °F

Same in both: Thermal Conductivity 17.5 W/m·K10.1 BTU/hr·ft·°F · Specific Heat Capacity 420 J/kg·K0.1 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 9.9 µm/m·K5.5 µin/in·°F · Latent Heat of Fusion 260 J/g112 BTU/lb · Max Service Temperature (continuous) 315°C599 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 2.9 % IACS · Electrical Resistivity 6×10⁻⁷ Ω·m23.6 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

78 / 100
72 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
42 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
45%

Weldability

55 / 100
50 / 100

Formability (cold)

60 / 100
25 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 52 MJ/kg22,356 BTU/lb · Embodied Carbon (primary production) 3.8 kg CO₂/kg · Embodied Water 120 L/kg14.4 gal/lb · Typical Recycled Content 55%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleS44627

S44627 Annealed vs S44627 As Welded — frequently asked

What is the difference between S44627 Annealed and S44627 As Welded?

S44627 Annealed and S44627 As Welded are two conditions of the same stainless steel grade, S44627: Annealed versus As Welded (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 345 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (Annealed versus as-welded deposit).

Which condition does FabDigit quote by default, Annealed or As Welded?

Annealed is the default S44627 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, S44627 Annealed or S44627 As Welded?

S44627 Annealed. Its weldability rates good (55/100) against fair (50/100) for S44627 As Welded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S44627 Annealed and S44627 As Welded side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.