FabDigitFabDigit

Stainless Steel S32803-ANN vs S32803-CD

Stainless Steel · S32803 temper comparison

S32803-ANN and S32803-CD are two conditions of the same stainless steel grade, S32803: ANN (annealed) versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. S32803-CD is the stronger of the two: yield strength 620 MPa (89.9 ksi) against 520 MPa (75.4 ksi) for S32803-ANN, about 19% more; tensile strength follows at 740 MPa (107 ksi) vs 640 MPa (92.8 ksi). In exchange, S32803-ANN is the more ductile: elongation 25% versus 18% for S32803-CD, and S32803-CD is harder (225 HB vs 195 HB).

S32803-ANNChoose it when the part is bent, formed or impact-loaded.

S32803-CDChoose it when strength drives the design.

S32803-ANN vs S32803-CD: properties

S32803-ANNS32803-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

640 MPa92.8 ksi
740 MPa107 ksi

Yield Strength (0.2% offset)

520 MPa75.4 ksi
620 MPa89.9 ksi

Elongation at Break

25%
18%

Reduction in Area

55%
45%

Shear Strength

400 MPa58 ksi
450 MPa65.3 ksi

Fatigue Strength (Endurance Limit)

340 MPa49.3 ksi
380 MPa55.1 ksi

Fracture Toughness (K_IC)

70 MPa·√m63.7 ksi·√in
55 MPa·√m50.1 ksi·√in

Charpy V-Notch Impact (RT)

50 J36.9 ft·lbf
35 J25.8 ft·lbf

Hardness, Brinell

195 HB
225 HB

Hardness, Rockwell B

92 HRB
99 HRB

Hardness, Vickers

205 HV
238 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.7 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
280°C536 °F

Same in both: Thermal Conductivity 16 W/m·K9.2 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 10.5 µm/m·K5.8 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -45°C-49 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

6.5×10⁻⁷ Ω·m25.6 µΩ·in
6.6×10⁻⁷ Ω·m26 µΩ·in

Same in both: Electrical Conductivity 2.6 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

82 / 100
80 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.15 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

28 / 100
32 / 100

Machinability Rating (AISI 1212 = 100 %)

35%
38%

Weldability

45 / 100
40 / 100

Formability (cold)

50 / 100
35 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 50 MJ/kg21,496 BTU/lb · Embodied Carbon (primary production) 4.5 kg CO₂/kg · Embodied Water 80 L/kg9.6 gal/lb · Typical Recycled Content 40%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleS32803

S32803-ANN vs S32803-CD — frequently asked

Is S32803-CD stronger than S32803-ANN?

Yes. S32803-CD has a typical yield strength of 620 MPa (89.9 ksi) against 520 MPa (75.4 ksi) for S32803-ANN — about 19% more. Tensile strength is 740 MPa (107 ksi) vs 640 MPa (92.8 ksi).

Which condition does FabDigit quote by default, ANN or CD?

ANN is the default S32803 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, S32803-ANN or S32803-CD?

S32803-ANN. Its weldability rates fair (45/100) against fair (40/100) for S32803-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S32803-ANN and S32803-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.