FabDigitFabDigit

Stainless Steel 1.4527-AC vs 1.4527-AW

Stainless Steel · 1.4527 temper comparison

1.4527-AC and 1.4527-AW are two conditions of the same stainless steel grade, 1.4527: AC (spheroidize annealed) versus AW (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 230 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (spheroidize annealed versus as-welded deposit). 1.4527-AW is the more ductile: elongation 30% versus 25% for 1.4527-AC.

1.4527-AWChoose it when the part is bent, formed or impact-loaded.

1.4527-AC vs 1.4527-AW: properties

1.4527-AC1.4527-AW

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elongation at Break

25%
30%

Reduction in Area

25%
30%

Compressive Strength

235 MPa34.1 ksi
230 MPa33.4 ksi

Fatigue Strength (Endurance Limit)

185 MPa26.8 ksi
175 MPa25.4 ksi

Fracture Toughness (K_IC)

95 MPa·√m86.5 ksi·√in
85 MPa·√m77.4 ksi·√in

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

165 HB
170 HB

Hardness, Rockwell B

86 HRB
87 HRB

Hardness, Vickers

175 HV
180 HV

Same in both: Elastic (Young's) Modulus 193 GPa28 Msi · Shear Modulus 75 GPa10.9 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Tensile Strength (Ultimate) 470 MPa68.2 ksi · Yield Strength (0.2% offset) 230 MPa33.4 ksi · Shear Strength 320 MPa46.4 ksi

Physical

Density and transition temperatures.

Same in both: Density 8 g/cm³0.29 lb/in³ · Melting Point (Solidus) 1,370°C2,498 °F · Liquidus Temperature 1,425°C2,597 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

12 W/m·K6.9 BTU/hr·ft·°F
12.1 W/m·K7 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 500 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 14.8 µm/m·K8.2 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.11×10⁻⁶ Ω·m43.7 µΩ·in
1.1×10⁻⁶ Ω·m43.3 µΩ·in

Same in both: Electrical Conductivity 1.6 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

60 / 100
68 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

25 / 100
27 / 100

Machinability Rating (AISI 1212 = 100 %)

28%
30%

Weldability

50 / 100
55 / 100

Formability (cold)

18 / 100
20 / 100

Same in both: Castability 70 / 100 · Brazeability / Solderability 45 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 78 MJ/kg33,534 BTU/lb · Embodied Carbon (primary production) 5.6 kg CO₂/kg · Embodied Water 220 L/kg26.4 gal/lb · Typical Recycled Content 55%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scale1.4527

1.4527-AC vs 1.4527-AW — frequently asked

What is the difference between 1.4527-AC and 1.4527-AW?

1.4527-AC and 1.4527-AW are two conditions of the same stainless steel grade, 1.4527: AC (spheroidize annealed) versus AW (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 230 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (spheroidize annealed versus as-welded deposit).

Which condition does FabDigit quote by default, AC or AW?

SA is the default 1.4527 condition in the FabDigit quote flow (neither AC nor AW). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 1.4527-AC or 1.4527-AW?

1.4527-AW. Its weldability rates good (55/100) against fair (50/100) for 1.4527-AC.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 1.4527-AC and 1.4527-AW side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.