FabDigitFabDigit

Zenite GF30 vs Zenite GF40

Polymer · Zenite grade comparison

Zenite GF30 and Zenite GF40 are two grades of the same polymer grade, Zenite: GF30 (30 % glass-fiber reinforced) versus GF40 (40 % glass-fiber reinforced). The chemistry is identical, so every difference below comes from the condition. Zenite GF40 is the stronger of the two: tensile strength 160 MPa (23.2 ksi) against 150 MPa (21.8 ksi) for Zenite GF30, about 7% more. In exchange, Zenite GF30 is the more ductile: elongation 1.8% versus 1.5% for Zenite GF40. Zenite GF30 is lighter (1.61 g/cm³ vs 1.7 g/cm³ for Zenite GF40) and Zenite GF40 is stiffer (18 GPa vs 15 GPa).

Zenite GF30Choose it when the part is bent, formed or impact-loaded, or when weight is the constraint.

Zenite GF40Choose it when strength drives the design.

Zenite GF30 vs Zenite GF40: properties

Zenite GF30Zenite GF40

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

15 GPa2.2 Msi
18 GPa2.6 Msi

Tensile Strength (Ultimate)

150 MPa21.8 ksi
160 MPa23.2 ksi

Elongation at Break

1.8%
1.5%

Flexural Strength

200 MPa29 ksi
215 MPa31.2 ksi

Flexural Modulus

14 GPa2 Msi
16 GPa2.3 Msi

Izod Impact, Notched

95 J/m1.8 ft·lbf/in
105 J/m2 ft·lbf/in

Same in both: Shear Modulus 1.6 GPa0.23 Msi · Poisson's Ratio 0.38 · Compressive Strength 60 MPa8.7 ksi · Shear Strength 45 MPa6.5 ksi · Hardness, Shore D 88 Shore D · Hardness, Rockwell M 75 HRM

Physical

Density and transition temperatures.

Density

1.61 g/cm³0.06 lb/in³
1.7 g/cm³0.06 lb/in³

Same in both: Melting Temperature (Tm) 335°C635 °F · Glass Transition (Tg) 125°C257 °F · Water Absorption (24 h) 0.02% · Water Absorption (Saturation) 0.1%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.4 W/m·K0.23 BTU/hr·ft·°F
0.3 W/m·K0.17 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
10 µm/m·K5.6 µin/in·°F

Heat Deflection Temp. @ 0.45 MPa

275°C527 °F
250°C482 °F

Heat Deflection Temp. @ 1.8 MPa

255°C491 °F
265°C509 °F

Same in both: Specific Heat Capacity 1,200 J/kg·K0.29 BTU/lb·°F · Max Service Temperature (continuous) 240°C464 °F · Min Service Temperature -50°C-58 °F · Limiting Oxygen Index 40% · Max Service Temperature (short-term) 280°C536 °F

Electrical

Conductivity and insulation.

Dielectric Constant (1 MHz)

3.9
3.3

Same in both: Electrical Resistivity 1×10¹³ Ω·m3.94×10²⁰ µΩ·in · Dielectric Strength 35 kV/mm889 V/mil · Dissipation Factor (1 MHz) 0.003 · Volume Resistivity 1×10¹⁵ Ω·cm · Surface Resistivity 1×10¹⁵ Ω · Comparative Tracking Index (CTI) 175 V

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Corrosion Resistance 92 / 100 · UV / Weathering Resistance 45 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

35 / 100
30 / 100

Same in both: Weldability 30 / 100 · Formability (cold) 20 / 100 · Polishability 40 / 100 · Mold Shrinkage 0.1% · Processing Melt Temperature (typ.) 345°C653 °F · Mold Temperature (typ.) 100°C212 °F

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 145 MJ/kg62,339 BTU/lb · Embodied Carbon (primary production) 7 kg CO₂/kg · Embodied Water 300 L/kg35.9 gal/lb · Typical Recycled Content 0%

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scale

Zenite GF30 vs Zenite GF40 — frequently asked

Is Zenite GF40 stronger than Zenite GF30?

Yes. Zenite GF40 has a typical tensile strength of 160 MPa (23.2 ksi) against 150 MPa (21.8 ksi) for Zenite GF30 — about 7% more.

Which grade does FabDigit quote by default, GF30 or GF40?

UF is the default Zenite condition in the FabDigit quote flow (neither GF30 nor GF40). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, Zenite GF30 or Zenite GF40?

Zenite GF30. Its machinability rates fair (35/100) against poor (30/100) for Zenite GF40.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Zenite GF30 and Zenite GF40 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.