Rigid 10K vs Tough 1000: properties

Rigid 10KTough 1000

Properties

Yield strength

75 MPa10.9 ksi
38 MPa5.5 ksi

Tensile strength

75 MPa10.9 ksi
50 MPa7.3 ksi

Elongation at break

3%
—

Elastic modulus (Young's)

6 GPa0.8 Msi
—

Density

1.55 g/cm³0.06 lb/in³
1.18 g/cm³0.04 lb/in³

Max service temp

100°C212 °F
80°C176 °F

Thermal conductivity

0.3 W/m·K
—

Weldability

3 / 100
5 / 100

Formability

3 / 100
5 / 100

Same in both: Electrical conductivity 0 % IACS · Machinability 40 / 100

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleFormlabs Rigid 10KFormlabs Tough 1000

Manufacturing and finishing

CapabilityRigid 10KTough 1000
Default conditionGlass Filled—
Relative cost$$$ Premium$$ Standard
Min. machined wall——
Best machined surface——

Both are offered for Injection molding and 3D printing. Both take the same 12 finishes: Chrome Plating (Plastic), Conductive Coating, Dyeing (Nylon), EMI Shielding Coating, Painting, Primer Coating, Soft Touch Coating, Spray Painting, Tinted Coating, UV Coating, Vacuum Metallization, Waterproof Coating.

Rigid 10K vs Tough 1000 — frequently asked

What is the difference between Rigid 10K and Tough 1000?

Rigid 10K and Tough 1000 are both polymer grades. On the shop floor, Tough 1000 sits in a lower cost tier (standard, $$) than Rigid 10K (premium, $$$).

Which is cheaper, Rigid 10K or Tough 1000?

Tough 1000 is the lower-cost material: it sits in the standard tier ($$) while Rigid 10K is premium ($$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

When should I choose Rigid 10K over Tough 1000?

Pick Tough 1000 when cost is the deciding factor.