PBT-GF30 GF30 vs PBT-GF30 GF30-HS
Polymer · PBT-GF30 grade comparison
PBT-GF30 GF30 and PBT-GF30 GF30-HS are two grades of the same polymer grade, PBT-GF30: GF30 (30% glass fiber, natural / uncolored, unmodified) versus GF30-HS. The chemistry is identical, so every difference below comes from the condition. PBT-GF30 GF30-HS runs hotter in service (150°C vs 130°C continuous).
PBT-GF30 GF30-HSChoose it when the part sees heat.
PBT-GF30 GF30 vs PBT-GF30 GF30-HS: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all polymer grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all polymer grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Izod Impact, Notched
Same in both: Elastic (Young's) Modulus 10 GPa1.5 Msi · Shear Modulus 3.6 GPa0.52 Msi · Poisson's Ratio 0.38 · Tensile Strength (Ultimate) 130 MPa18.9 ksi · Elongation at Break 3% · Compressive Strength 130 MPa18.9 ksi · Compressive Modulus 8.5 GPa1.2 Msi · Flexural Strength 200 MPa29 ksi · Flexural Modulus 9 GPa1.3 Msi · Shear Strength 60 MPa8.7 ksi · Fracture Toughness (K_IC) 3.5 MPa·√m3.2 ksi·√in · Hardness, Shore D 85 Shore D · Hardness, Rockwell M 90 HRM · Hardness, Rockwell R 120 HRR
Physical
Density and transition temperatures.
Same in both: Density 1.53 g/cm³0.06 lb/in³ · Melting Temperature (Tm) 225°C437 °F · Glass Transition (Tg) 50°C122 °F · Water Absorption (24 h) 0.06% · Water Absorption (Saturation) 0.35%
Thermal
How each material carries heat and how hot it can run.
Max Service Temperature (continuous)
Max Service Temperature (short-term)
Same in both: Thermal Conductivity 0.25 W/m·K0.14 BTU/hr·ft·°F · Specific Heat Capacity 1,400 J/kg·K0.33 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 25 µm/m·K13.9 µin/in·°F · Min Service Temperature -40°C-40 °F · Heat Deflection Temp. @ 0.45 MPa 215°C419 °F · Heat Deflection Temp. @ 1.8 MPa 207°C405 °F · Vicat Softening Point (B50) 200°C392 °F · Limiting Oxygen Index 22%
Electrical
Conductivity and insulation.
Same in both: Electrical Resistivity 1×10¹⁴ Ω·m3.94×10²¹ µΩ·in · Dielectric Strength 30 kV/mm762 V/mil · Dielectric Constant (1 MHz) 3.7 · Dissipation Factor (1 MHz) 0.02 · Volume Resistivity 1×10¹⁶ Ω·cm · Surface Resistivity 1×10¹⁵ Ω · Comparative Tracking Index (CTI) 550 V
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Same in both: Corrosion Resistance 82 / 100 · UV / Weathering Resistance 30 / 100
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Weldability
Melt Flow Rate
Same in both: Formability (cold) 10 / 100 · Polishability 30 / 100 · Mold Shrinkage 0.4% · Processing Melt Temperature (typ.) 260°C500 °F · Mold Temperature (typ.) 80°C176 °F
Sustainability
Primary-production footprint per kilogram.
Same in both: Embodied Energy (primary production) 85 MJ/kg36,543 BTU/lb · Embodied Carbon (primary production) 4.4 kg CO₂/kg · Embodied Water 200 L/kg24 gal/lb · Typical Recycled Content 5%
Strength versus weight
Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
PBT-GF30 GF30 vs PBT-GF30 GF30-HS — frequently asked
What is the difference between PBT-GF30 GF30 and PBT-GF30 GF30-HS?
PBT-GF30 GF30 and PBT-GF30 GF30-HS are two grades of the same polymer grade, PBT-GF30: GF30 (30% glass fiber, natural / uncolored, unmodified) versus GF30-HS. The chemistry is identical, so every difference below comes from the condition. PBT-GF30 GF30-HS runs hotter in service (150°C vs 130°C continuous).
Which grade does FabDigit quote by default, GF30 or GF30-HS?
GF30 is the default PBT-GF30 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.
Which is easier to machine, PBT-GF30 GF30 or PBT-GF30 GF30-HS?
PBT-GF30 GF30-HS, by a small margin. Both rate good for machinability — 60/100 against 55/100 for PBT-GF30 GF30; for welding the order is PBT-GF30 GF30 first (fair, 45/100) then PBT-GF30 GF30-HS (fair, 40/100).