EPP CD and EPP45 are two grades of the same polymer grade, EPP: CD (cold drawn) versus EPP45 (EPP 45 g/L). The chemistry is identical, so every difference below comes from the condition. EPP45 is the stronger of the two: tensile strength 0.6 MPa (0.087 ksi) against 0.36 MPa (0.0522 ksi) for EPP CD, about 67% more. EPP45 is the more ductile: elongation 20% versus 15% for EPP CD. EPP CD is lighter (0.03 g/cm³ vs 0.05 g/cm³ for EPP45) and EPP45 is stiffer (0.01 GPa vs 0 GPa).

EPP CDChoose it when weight is the constraint.

EPP45Choose it when strength drives the design, or when the part is bent, formed or impact-loaded.

EPP CD vs EPP45: properties

EPP CDEPP45

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0 GPa5.08×10⁻⁴ Msi
0.01 GPa0 Msi

Tensile Strength (Ultimate)

0.36 MPa0.05 ksi
0.6 MPa0.09 ksi

Elongation at Break

15%
20%

Compressive Strength

0.21 MPa0.03 ksi
0.38 MPa0.06 ksi

Compressive Modulus

0 GPa4.35×10⁻⁴ Msi
0.01 GPa7.25×10⁻⁴ Msi

Flexural Strength

0.4 MPa0.06 ksi
0.7 MPa0.1 ksi

Flexural Modulus

0.01 GPa7.98×10⁻⁴ Msi
0.01 GPa0 Msi

Shear Strength

0.18 MPa0.03 ksi
0.3 MPa0.04 ksi

Compression Set (22 h, 70 °C)

13%
11%

Same in both: Poisson's Ratio 0.05

Physical

Density and transition temperatures.

Density

0.03 g/cm³0 lb/in³
0.05 g/cm³0 lb/in³

Same in both: Melting Temperature (Tm) 155°C311 °F · Glass Transition (Tg) -12°C10 °F · Water Absorption (24 h) 0.6% · Water Absorption (Saturation) 2%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.04 W/m·K0.02 BTU/hr·ft·°F
0.04 W/m·K0.02 BTU/hr·ft·°F

Max Service Temperature (continuous)

95°C203 °F
100°C212 °F

Limiting Oxygen Index

19%
18%

Same in both: Specific Heat Capacity 1,900 J/kg·K0.45 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 90 µm/m·K50 µin/in·°F · Min Service Temperature -40°C-40 °F · Max Service Temperature (short-term) 130°C266 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1,000 Ω·m3.94×10¹⁰ µΩ·in
1×10¹³ Ω·m3.94×10²⁰ µΩ·in

Volume Resistivity

100,000 Ω·cm
1×10¹⁵ Ω·cm

Surface Resistivity

100,000 Ω
1×10¹⁴ Ω

Same in both: Dielectric Constant (1 MHz) 1.08 · Dissipation Factor (1 MHz) 4×10⁻⁴

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

55 / 100
25 / 100

Same in both: Corrosion Resistance 90 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

57 / 100
60 / 100

Weldability

50 / 100
55 / 100

Formability (cold)

33 / 100
35 / 100

Same in both: Mold Shrinkage 2.5%

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 100 MJ/kg42,992 BTU/lb · Embodied Carbon (primary production) 3.8 kg CO₂/kg · Embodied Water 130 L/kg15.6 gal/lb · Typical Recycled Content 10%

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scale

EPP CD vs EPP45 — frequently asked

Is EPP45 stronger than EPP CD?

Yes. EPP45 has a typical tensile strength of 0.6 MPa (0.087 ksi) against 0.36 MPa (0.0522 ksi) for EPP CD — about 67% more.

Which grade does FabDigit quote by default, CD or EPP45?

EPP30 is the default EPP condition in the FabDigit quote flow (neither CD nor EPP45). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, EPP CD or EPP45?

EPP45. Its weldability rates good (55/100) against fair (50/100) for EPP CD.