FabDigitFabDigit

Cedar vs Southern Yellow Pine

Natural Material · grade comparison

Cedar and Southern Yellow Pine are both natural material grades. Southern Yellow Pine is the stronger of the two: tensile strength 80 MPa (11.6 ksi) against 55 MPa (7.98 ksi) for Cedar, about 45% more. Southern Yellow Pine is the more ductile: elongation 1.2% versus 1% for Cedar. Cedar is lighter (0.37 g/cm³ vs 0.62 g/cm³ for Southern Yellow Pine) and Southern Yellow Pine is stiffer (11.5 GPa vs 7.7 GPa). On the shop floor, Cedar machines more easily (excellent vs very good) and Southern Yellow Pine sits in a lower cost tier (budget, $) than Cedar (premium, $$$).

CedarChoose it when weight is the constraint, or when the part is machined in volume.

Southern Yellow PineChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

Cedar vs Southern Yellow Pine: properties

CedarSouthern Yellow Pine

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

7.7 GPa1.1 Msi
11.5 GPa1.7 Msi

Shear Modulus

0.5 GPa0.07 Msi
0.9 GPa0.13 Msi

Poisson's Ratio

0.37
0.33

Tensile Strength (Ultimate)

55 MPa8 ksi
80 MPa11.6 ksi

Elongation at Break

1%
1.2%

Compressive Strength

31 MPa4.6 ksi
44 MPa6.4 ksi

Flexural Strength

52 MPa7.5 ksi
80 MPa11.6 ksi

Shear Strength

7 MPa0.99 ksi
10 MPa1.4 ksi

Fracture Toughness (K_IC)

0.4 MPa·√m0.36 ksi·√in
0.38 MPa·√m0.35 ksi·√in

Physical

Density and transition temperatures.

Density

0.37 g/cm³0.01 lb/in³
0.62 g/cm³0.02 lb/in³

Porosity

74%
60%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.09 W/m·K0.05 BTU/hr·ft·°F
0.16 W/m·K0.09 BTU/hr·ft·°F

Specific Heat Capacity

1,600 J/kg·K0.38 BTU/lb·°F
1,800 J/kg·K0.43 BTU/lb·°F

Max Service Temperature (continuous)

65°C149 °F
80°C176 °F

Same in both: Thermal Expansion (CTE, 20–100 °C) 4 µm/m·K2.2 µin/in·°F · Min Service Temperature -60°C-76 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10⁹ Ω·m3.94×10¹⁶ µΩ·in
1×10⁷ Ω·m3.94×10¹⁴ µΩ·in

Dielectric Strength

1.5 kV/mm38.1 V/mil
5 kV/mm127 V/mil

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

80 / 100
30 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

90 / 100
80 / 100

Same in both: Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

9 MJ/kg3,654 BTU/lb
9 MJ/kg3,869 BTU/lb

Embodied Carbon (primary production)

0.45 kg CO₂/kg
0.3 kg CO₂/kg

Typical Recycled Content

0%
2%

Same in both: Embodied Water 500 L/kg59.9 gal/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

149 kN·m/kg
129 kN·m/kg

Specific Stiffness (E / density)

20.8 MN·m/kg
18.5 MN·m/kg

Thermal Diffusivity

0.2 mm²/s
0.1 mm²/s

Same in both: Thermal Shock Resistance Index 0

Strength versus weight

Yield strength against density for every natural material grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

Manufacturing and finishing

CapabilityCedarSouthern Yellow Pine
Default condition——
Relative cost$$$ Premium$ Budget
Min. machined wall——
Best machined surface——

Cedar vs Southern Yellow Pine — frequently asked

Is Southern Yellow Pine stronger than Cedar?

Yes. Southern Yellow Pine has a typical tensile strength of 80 MPa (11.6 ksi) against 55 MPa (7.98 ksi) for Cedar — about 45% more.

Which is cheaper, Cedar or Southern Yellow Pine?

Southern Yellow Pine is the lower-cost material: it sits in the budget tier ($) while Cedar is premium ($$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, Cedar or Southern Yellow Pine?

Cedar. Its machinability rates excellent (90/100) against very good (80/100) for Southern Yellow Pine.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Cedar and Southern Yellow Pine side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.